Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 54.4 - 71.1 °C | 130 - 160 °F | |
PTS Trilac® FR3800-V Flame Retardant ABS Resin, RoHS Compliant Contains UV absorber.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 54.4 - 65.6 °C | 130 - 150 °F | |
PolyOne Lubri-Tech™ AS-20GF/05T Acrylonitrile Butadiene Styrene (ABS), Glass Filled, PTFE Lubricated
(discont Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 54.4 - 120 °C | 130 - 248 °F | Average value: 86.4 °C Grade Count:41 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Mold Temperature | 54.4 - 71.1 °C | 130 - 160 °F | |
TPI Porene® ABS-AN450 Flame Retardant ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 54.4 - 82.2 °C | 130 - 180 °F | |
Clariant 6618G15 HSL UV Black Nylon 66, 15% Glass Fiber, Impact Modified, UV and Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Mold Temperature | 54.4 - 65.6 °C | 130 - 150 °F | 45 secs De-mold Time |
Dow SPECTRIM™ MM310 Reaction Moldable Polymer SPECTRIM™ MM 310 reaction moldable polymer is a three-component, fast-reacting, low viscosity polycarbamate system ideally suited for mat molding of structural composites. The structural reaction .. |
|||
Mold Temperature | 54.4 - 76.7 °C | 130 - 170 °F | |
Polymer Resources PPX-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |