Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical AF342 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical AF345 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical HF380G ABS, High Flow Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical HG193S ABS, High Flow, Chemical Resistance Feature: Injection Molding, High Flow, Chemical ResistanceApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical HI100X ABS, High Impact, Semi-Transparency, Flexible Feature: Injection Molding, High Impact, Semi-Transparency, FlexibleApplication: Artificial Nails, Miscellaneous Goods)CAS No. 9010-94-0Information provided by LG Chemical |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | |
LG Chemical KEYFLEX TO-1175A Thermoplastic Olefin for Extrusion, 75A Hardness KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber .. |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL GP1007F Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL HI5205R PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL TE5107 PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL TE5108H PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical AF308 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical AF360 ABS, TBBA-free Flame Retardant Feature: Injection Molding, TBBA-free Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information provided b.. |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL GP3102Y PP+MF10%, High Impact, High Flow Description: Injection Molding, PP+MF10%, General Purpose, High Impact, High FlowApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemica.. |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL HF5157 PP+Rubber+MF, High Flow and Stiffness, High Impact Description: Injection Molding, PP+Rubber+MF, High Flow and Stiffness, High Impact, Good Weatherability, Scratch ResistanceApplication: Automotive Exterior (Slim wall Bumper Fascia)Information provi.. |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL HR2100D PP+GF17% Description: Injection Molding, PP+GF17%, General PurposeApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0 and 165997-17-3Information provided by LG Chemical |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL MC4352 PP+Rubber+MF Description: Injection Molding, PP+Rubber+MF, Good Dimensional Stability, Scratch resistance, Good Weatherability, High ImpactApplication: Automotive Exterior (Sill Side Molding, Door Garnish)CAS: 9.. |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | |
Lehmann & Voss LUVOCOM® 100-7846 Thermoplastic polyurethane, with aramid reinforcement Applications: Improved friction and wear behaviour. Emergency running property.dynamic stressBearings, sleeves, sliding elements, chair rollers, handles.Information provided by Lehmann & Voss & Co.K.. |
|||
Nozzle Temperature | 220 - 230 °C | 428 - 446 °F | Injection Molding |
Stellarchem AB760LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 220 - 230 °C | 428 - 446 °F | Injection Molding |
Stellarchem AB835EM TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 220 - 230 °C | 428 - 446 °F | Injection Molding |
Stellarchem GP-975 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 220 - 230 °C | 428 - 446 °F | Injection Molding |
Stellarchem LP-855 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 220 - 230 °C | 428 - 446 °F | Injection Molding |
Stellarchem MP-8001 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 190 - 230 °C | 374 - 446 °F | |
Teknor Apex Uniprene® 7010-64NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Nozzle Temperature | 190 - 230 °C | 374 - 446 °F | |
Teknor Apex Uniprene® UN-1140A Thermoplastic Elastomer Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Nozzle Temperature | 190 - 230 °C | 374 - 446 °F | |
Teknor Apex Uniprene® UN-2028A UMB Thermoplastic Elastomer Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Nozzle Temperature | 190 - 230 °C | 374 - 446 °F | |
Teknor Apex Uniprene® UN-7100-87 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | |
Tisan TISLAMID® 6 30% Glass Fiber Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | |
Tisan TISLAMID® 6 30% Glass Filled Impact Modified, Heat Stabilized Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | |
Tisan TISLAMID® 6 30% Mineral Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical MA201 ABS, Low Gloss Feature: Injection Molding, Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |