Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 310 - 327 °C | 590 - 620 °F | |
Oxford Polymers PC 30CF-925 Black PC, 30% Carbon Fiber Reinforced Product Description: Glass Fiber (30% Reinforced), PBT injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents Special Characteristics: High Str.. |
|||
Nozzle Temperature | 299 - 327 °C | 570 - 620 °F | |
Ravago Manufacturing Americas Hylex® P1007L Polycarbonate Information provided by Ravago |
|||
Nozzle Temperature | 299 - 327 °C | 570 - 620 °F | |
Ravago Manufacturing Americas Hylex® P1307L Polycarbonate Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Nozzle Temperature | 254 - 327 °C | 489 - 620 °F | Average value: 298 °C Grade Count:47 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Nozzle Temperature | 304 - 327 °C | 580 - 620 °F | |
LTL Color Compounds ColorFast® PC60 Polycarbonate 6 melt extrusion gradeAll information provided by LTL Color Compounders, Inc. |
|||
Nozzle Temperature | 304 - 327 °C | 580 - 620 °F | |
LTL Color Compounds ColorFast® PCGF110 Polycarbonate, 10% Glass-Filled High modulus 10% glass-filled polycarbonate, V2-rated, general purposeAll information provided by LTL Color Compounders, Inc. |
|||
Nozzle Temperature | 299 - 327 °C | 570 - 621 °F | |
Styron CALIBREâ„¢ 2061-6 Polycarbonate Resin Overview: CALIBREâ„¢ 2061-6 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-6 provides excellent heat resistance, impact strength, .. |
|||
Nozzle Temperature | 304 - 327 °C | 580 - 620 °F | |
LTL Color Compounds ColorFast® FRPC310 Polycarbonate, Flame-Retarded V0-rated 10% glass-filled polycarbonate, excellent impact strengthAll information provided by LTL Color Compounders, Inc. |