Processing Properties Metric English Comments
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength  (d
Melamine/phenolic molding compound, inorganically filled, glass fiber reinforced, good temperature stability, high level of mechanical properties, copper adhesive, flammability UL 94/V-0/1.6 mm (not..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 13 Phenolic Formaldehyde Resin, UL Listed  (discontinued **)
Phenolic molding compound, inorganically mica filled, heat resistance, good electrical properties, UL listed molding compound 0.75 mm/V-1 (NC), 3 mm/V-0, standardized molding compound.Application ar..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 31.9 Phenolic Formaldehyde Resin, Ammonia Free  (discontinued **)
Phenolic molding compound, mainly organically filled, ammonia free, standardized molding compound.Application areas: Parts for electrical and telecommunications technology, motor vehicle ignition sy..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 51 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets  (discontinued **)
Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Contact support power switch, switch..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 84 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets, High Mechanical Strength &
Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Contact support power switch, moldin..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 1107 Phenolic Formaldehyde Resin, Low Shrinkage, Resistant to High Temperatures  (disconti
Phenolic molding compound, inorganically filled, glass fiber reinforced, high heat resistance, low heat expansion coefficient, highest resistance to pressure, high dimensional stability.Application ..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 1141 Phenolic Formaldehyde Resin, High Surface Quality, Resistant to High Temperatures, Dishwasher Proof
Phenolic molding compound, inorganically/organically filled, glass fiber reinforced, increased heat resistance, hot steam and hot water resistant (not suitable for use of higher voltage).Application..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 2535 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof  (discontinued **
Phenolic molding compound, inorganically/organically filled, average heat resistant, steam resistant, dish washer proof, high surface quality.Application areas: Fittings for ovens and dishwashers, t..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 4109 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free
Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, low shrinkage, high mechanical strength, U..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 6507 Phenolic Formaldehyde Resin, Elasticized, Low Shrinkage, Resistant to High Temperatures, High Mechanical Strength
Phenolic molding compound, inorganically filled, glass fiber reinforced, elastomer modified, galvanizable, heat resistant, good media resistance, high dimensional stability at raised temperature, hi..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 7592 Phenolic Formaldehyde Resin, Galvanized, Conductive  (discontinued **)
Phenolic molding compound, inorganically/organically filled. Shrinkage fies compatible to values of UP 3310 and PF 2560. Electroplateable.Application areas: Chromium plated oven strips.Information..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 13591 Phenolic Formaldehyde Resin, High Surface Quality, UL Listed  (discontinued **)
Phenolic molding compound, mainly organically filled, very soft flow for large molds, UL listed molding compound 1.5 mm/V-1 (BK), 3.0 mm/V-0 (BK).Application areas: Pan handles, various applications..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 14694 Phenolic Formaldehyde Resin, High Surface Quality  (discontinued **)
Phenolic molding compound, mainly organically filled, very soft flow for large molds.Application areas: Housing parts, heat shields, cookware fittings.Information provided by Bak AGBak AG became a p..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ 151733 Phenolic Formaldehyde Resin  (discontinued **)
Phenolic molding compound, mainly organically filled, standard molding compound for normal stress.Application areas: Contact strips.Information provided by Bak AGBak AG became a part of Hexion in 20..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ 460124 Phenolic Formaldehyde Resin  (discontinued **)
Phenolic molding compound, mainly organically filled, standard molding compound for normal stress.Application areas: Cookware fittings, electric devices.Information provided by Bak AGBak AG became a..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ X24 Phenolic Formaldehyde Resin  (discontinued **)
Phenolic molding compound, mainly organically filled.Application areas: Operating controls, housing parts, lamp holders.Information provided by Bak AGBak AG became a part of Hexion in 2005.
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ X30 Phenolic Formaldehyde Resin  (discontinued **)
Phenolic molding compound, reinforced with cotton and sisal fibers, increased notched impact strength.Application areas: Covers for electrical and electromagnetic devices.Information provided by Bak..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ X65 Phenolic Formaldehyde Resin, UL Listed  (discontinued **)
Phenolic molding compound, inorganically/organically filled, good heat-resistance and dimensional stability, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Oven strips.Information..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 2874 Phenolic Formaldehyde Resin, Low Shrinkage, Improved Electrical Properties, UL Listed, High Mechanical Strength
Phenolic molding compound, inorganically filled, glass fiber reinforced, increased mechanical strength, increased temperature stability, low water absorption, good dimensional stability, UL listed m..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 6501 Phenolic Formaldehyde Resin, Low Shrinkage
Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistant.Application areas: Thermally and dyna..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 4010 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage  (disconti
Glass fiber reinforced and inorganically filled molding compound. High heat resistance, reduced molding shrinkage, good chemical resistance and mechanical properties.Application areas: Switch housi..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 4111 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free, Copper Adhesive
Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, high mechanical strength, copper-adhesive,..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 8052 Phenolic Formaldehyde Resin, Resistant to High Temperatures  (discontinued **)
Phenolic molding compound, glass fiber reinforced and inorganically filled. Excellent heat resistance with respect to surface finish and mechanical properties.Application areas: Pan handles, heat r..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 83 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets  (discontinued **)
Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Switch covers, rolls, handle casings..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 1142 Phenolic Formaldehyde Resin, High Mechanical Strength  (discontinued **)
Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability, good mechanical properties.Application areas: Insulating flanges, sealings, pulleys.Information p..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 2560 Phenolic Formaldehyde Resin, High Surface Quality, For Electrostatic Coating, UL Listed &n
Phenolic molding compound, inorganically/organically filled, average heat resistant, high surface quality, lower water absorption than PF 31, minimal distortion, UL listed molding compound 1.5 mm/V-..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 2836 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed &nbs
Phenolic molding compound, inorganically/organically filled, increased heat resistance, increased tracking resistance, low shrinkage and post shrinkage, improved electrical properties, UL listed mol..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 2855 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage, For Electrostatic Coating, Dishwasher Proof, UL Listed
Phenolic molding compound, inorganically/organically filled, heat resistant up to 250°C, hot steam and hot water resistant, high surface quality, for electrostatic coating, UL listed molding compou..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 4155 Phenolic Formaldehyde Resin, Resistant to High Temperatures, Improved Electrical Properties, Low Shrinkage, High Mechanical Strength
Phenolic molding compound, inorganically filled, glass fiber reinforced, good media and temperature resistance. Conditioned Cu-adhesion.Application areas: Commutators (fuel pumps, actuators, starte..
Nozzle Temperature 80.0 - 100 °C
176 - 212 °F
Injection molding
Hexion Bakelite™ PF 4260 Phenolic Formaldehyde Resin, Resistant to High Temperatures, Improved Electrical Properties, Low Shrinkage, High Mechanical Strength
Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistantApplication areas: Commutators (starte..