Processing Properties Metric English Comments
Nozzle Temperature 160 - 171 °C
320 - 340 °F
RheTech Products E204-01 High Density Polyethylene, Black
Applications: Electrical housingsUnderhood componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 160 - 193 °C
320 - 379 °F
PolyOne Versaflex™ CL2000X Thermoplastic Elastomer (TPE)
Versaflex™ CL2000X is an ultra-soft TPE designed for use in injection molding applications where exceptional clarity and an extremely soft feel are desired. - Tactile Feel - Ultra-Soft - Water Clar..
Nozzle Temperature 160 - 299 °C
320 - 570 °F
Average value: 199 °C Grade Count:75
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim..
Nozzle Temperature 160 - 185 °C
320 - 365 °F
Huntsman AVALON® 75 ABX Thermoplastic Polyurethane
Introduction: AVALON 70 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 70 ABX is part of the AVALON Perform Range and offers a specially designed,..
Nozzle Temperature 160 - 185 °C
320 - 365 °F
Huntsman AVALON® 65 ABX Thermoplastic Polyurethane
Introduction: AVALON 65 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 65 ABX is part of the AVALON Perform Range and offers a specially designed,..
Nozzle Temperature 160 - 185 °C
320 - 365 °F
Huntsman AVALON® 70 ABX Thermoplastic Polyurethane
Introduction: AVALON 70 ABX is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 70 ABX is part of the AVALON Perform Range and offers a speci..
Nozzle Temperature 160 - 170 °C
320 - 338 °F
Huntsman IROGRAN® A 60 E 4902 TPU-Polyester
Introduction: IROGRAN A 60 E 4902 is a soft, high performance polyester based thermoplastic polyurethane intended for extrusion and molding applications. IROGRAN A 60 E 4902 is part of the HUNTSMAN ..
Nozzle Temperature 160 °C
320 °F
SK Chemicals SKYTHANE® T850A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Nozzle Temperature 160 - 171 °C
320 - 340 °F
RheTech Products E204-00 High Density Polyethylene, Natural
Applications: Electrical housingsUnderhood componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.