Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Velocity | 200 mm/sec | 7.87 in/sec | |
Ineos ABS Centrex® 813 ASA+AES Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba.. |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | |
Ineos ABS Centrex® 811 ASA Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba.. |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | |
Ineos ABS Lustran® 130 Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Injection moldingSheet extrusionBlow moldingThermoforming |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Styrolution Luran® HD 20 SAN Luran HD 20 is an easy-flow grade of SAN especially designed for the medical market. It is suitable for moldings with very thin walls and / or adverse flow length to wall ratio. It features very goo.. |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Styrolution Luran® HH-120 Alpha-Methylstyrene Acrylonitrile Luran HH-120 is a grade of AMSAN with high heat resistance and improved mechanical strength. It is suitable for injection molding and extrusion applications and can be used as a modifier for high he.. |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | Injection molding |
Styrolution Luran® S 776 SE ASA Luran S 776 SE is a general purpose extrusion ASA grade with good toughness and strength, used for sheet and profile extrusions.Information provided by STYROLUTION, which is a joint venture between .. |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Styrolution PS 147F GPPS Styrolution PS 147F is a highly transparent GPPS grade. It gives excellent mechanical and heat resistance properties while providing with easy processability and short cycle time.Medium FlowEasy pro.. |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Styrolution PS 168 N/L GPPS Styrolution PS 168N/L is a high molecular weight, heat resistant grade with high mechanical strength. It is suitable for physically or chemically expanded extruded sheet. It is also suitable for use.. |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Styrolution PS 485N HIPS Styrolution PS 485N is a high impact grade of polystyrene for extruded sheets with a matte surface.Matte SurfaceUL 94 HBInformation provided by Styrolution |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Styrolution Terluran® GP-25 ABS Terluran GP-25 is an easy-flow, general purpose injection molding grade with high resistance to impact and heat distortion; intended for a wide range of applications, particularly in the housings se.. |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Covestro Apec® 2097 Polycarbonate Easy flowingeasy to demoldUV-stabilizedsoftening temperature (VST/B 120)=202 °CPreprocessingMax. Water content |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Covestro Apec® DP1-9389/5 Polycarbonate Developmental producteasy flowingeasy to demoldsoftening temperature (VST/B 120)=218 °CPreprocessingMax. Water content |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Covestro Apec® FR1892 High-Heat Polycarbonate This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along.. |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Covestro Makroblend® DP UT5005 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding gradeMakroblend DP UT5005* provides an outstanding balance of low-temperature impact strength and flowability beside e.. |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Covestro Makroblend® KU 2-7915 Polycarbonate + PBT, Impact Grade ISO 7792-1-PC/PBT,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradeexcellent toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessingMax. Water content |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Covestro Makroblend® KU 2-7940 Polycarbonate + PBT, Impact Grade Developmental productISO 7792-1-PC/PBT,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradehigh toughness at low temperaturesunreinforcedPreprocessingMax. Water content |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Covestro Makroblend® S 7916/2 Polycarbonate + PBT, Impact Grade ISO 7792-1-PBT/PC,MHPR,-020(PBT+PC)-blendsimpact modifiedInjection molding gradeexcellent chemical resistancehigh toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessing.. |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Covestro Makrolon® 1881 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Impact modified• Imp.. |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Covestro Makrolon® 2556 Polycarbonate MVR (300 °C/1.2 kg) 14 cm3/10 minEasy releaseGood hydrolysis resistanceInjection moldingAvailable in transparentTranslucent and opaque colorsFood contact gradePreprocessingMax. Water content |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Covestro Makrolon® 2558 Polycarbonate ISO 7391-PC,MR,(,,)-18-9MVR (300 °C/1.2 kg) 14.5 cm3/10 minMedical devicessuitable for ETO and steam sterilization at 121 °CComplies with the requirements of FDA-modified ISO 10993-1 and USP Class.. |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Covestro Makrolon® 2652 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Covestro Makrolon® 2856 Polycarbonate ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAva.. |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Covestro Makrolon® 6255 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Lo.. |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Covestro Makrolon® 6455 Polycarbonate, Flame Retardant Grade MVR (300 °C/1.2 kg) 12.5 cm3/10 minUL 94V-0/3.0 mmeasy releaseinjection moldingavailable in transparenttranslucent and opaque colorsPreprocessingMax. Water content |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Covestro Makrolon® LED2045 Polycarbonate ISO 7391-PC,MRT,(,,)-24-9Global gradeMVR (250 °C/2.16 kg) 16.5 cm3/10minLight guidesPC with highest transmissionLow viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable .. |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Covestro Makrolon® LQ3147 Polycarbonate ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minOptical lensHigh viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in clear tints .. |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Covestro Makrolon® Rx2430 Polycarbonate ISO 7391-PC,M,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minMedical devicessuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modified ISO 10993-1 an.. |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Covestro Makrolon® 6487 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minFlame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmMedium viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 2.. |
|||
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Covestro Makrolon® Rx2635 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Med.. |