Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 257 - 271 °C | 495 - 520 °F | |
Teknor Apex Beetle® 102 Nylon 66, Unreinforced, Nucleated Notes: Nucleated for fast cycling; Improved strength and rigidity; FMVSS Flammability: Passes, FMVSS 302Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Middle Barrel Temperature | 257 - 271 °C | 495 - 520 °F | |
Teknor Apex Beetle® 140 BH Nylon 66, Glass Bead Reinforced Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Middle Barrel Temperature | 257 - 274 °C | 495 - 525 °F | |
Teknor Apex Chemlon® 100 L Nylon 66, Unreinforced Notes: Internally and externally lubricated; General Purpose; Double-lubricated for improved part ejection and machine feed Processing Method: Injection Molding Forms: PelletsInformation Provided by.. |
|||
Middle Barrel Temperature | 257 - 274 °C | 495 - 525 °F | |
Teknor Apex Chemlon® 100 Nylon 66, Unreinforced Features: Basic nylon 66 with internal lubrication. Widely used for automotive, electronic and appliance applications. Processing Method: Injection Molding Forms: Pellets Automotive Specifications: .. |
|||
Middle Barrel Temperature | 257 - 271 °C | 495 - 520 °F | |
Teknor Apex Chemlon® 100 W Nylon 66, Unreinforced Notes: MoS2 modified; Molybdenum disulphide modified to provide self-lubrication and low friction to parts subjected to wear and abrasion. FMVSS Flammability: Passes, FMVSS 302Processing Method: Inj.. |
|||
Middle Barrel Temperature | 257 - 274 °C | 495 - 525 °F | |
Teknor Apex Chemlon® 104 Nylon 66, Impact Grade Notes: Medium-Impact; General Purpose; Impact modified to provide excellent toughness Processing Method: Injection Molding Forms: Pellets Automotive Specifications: Chrysler MS-DB41 CPN3992 Color: W.. |
|||
Middle Barrel Temperature | 257 - 271 °C | 495 - 520 °F | |
Teknor Apex Chemlon® 109 Nylon 66, Impact Grade Notes: High-Impact; Exceptional impact strength, especially at low temperatures; FMVSS Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets Automotive Specifications: .. |
|||
Middle Barrel Temperature | 257 - 271 °C | 495 - 520 °F | |
Teknor Apex Chemlon® 113 GH Nylon 66, 13% Short Glass Fiber Reinforced Features: Good creep Resistance; Good stiffness; Good dimensional stability; High strength; Heat stabilized Processing Method: Injection Molding Forms: Pellets Automotive Specifications: Chrysler MS.. |
|||
Middle Barrel Temperature | 257 - 271 °C | 495 - 520 °F | |
Teknor Apex Chemlon® 143 G Nylon 66, 43% Short Glass Fiber Reinforced Notes: Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets FMVSSInformation Provided by Teknor Apex |
|||
Middle Barrel Temperature | 257 - 274 °C | 495 - 525 °F | |
Teknor Apex Chemlon® 140 MH Nylon 66, 40% Mineral Reinforced Notes: 40% Mineral; High rigidity with exceptional control of warpage and surface sink marks; Excellent for large parts; Fast cycling Features: Fast Molding Cycle; High Rigidity; Heat Stabilized; Lo.. |