Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 185 - 196 °C | 365 - 385 °F | |
Polymer Resources AC-GP2-TFE5 Acetal Copolymer, 5% PTFE Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 185 - 218 °C | 365 - 424 °F | |
Ineos Nova Zylar® 390 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features: Excellent clarityHigh flexural modulusGood toughness and elongationStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specification.. |
|||
Middle Barrel Temperature | 185 - 218 °C | 365 - 424 °F | |
Ineos Nova Zylar® 330 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:Clarity and stiffness Good heat distortion resistance Styrenic processing advantages Excellent property retention after gamma and ETO sterilization Meets USP XXIII specifications for Class .. |
|||
Middle Barrel Temperature | 185 °C | 365 °F | |
Huntsman IROGRAN® A 75 P 4655 N TPU-Polyester Introduction: IROGRAN A 75 P 4655 N is a black colored polyether based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 75 P 4655 N is a part of the HUNTSMAN injecti.. |
|||
Middle Barrel Temperature | 185 - 200 °C | 365 - 392 °F | Injection Molding |
Ineos ABS Lustran® SAN DN59 SAN, Soft-Flow Grade Lustran® SAN DN59 resin is a soft-flow grade of transparent SAN (styrene acrylonitrile) thermoplastic. It has been designed for use in compounding and thin-wall injection molded applications. Lus.. |
|||
Middle Barrel Temperature | 185 - 195 °C | 365 - 383 °F | Extrusion |
Huntsman IROGRAN® A 91 P 4945 TPU-Polyester Introduction: IROGRAN A 91 P 4945 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 91 P 4945 is part of the HUNTSMAN technical ext.. |
|||
Middle Barrel Temperature | 185 - 200 °C | 365 - 392 °F | |
Lavergne VYSTYRENE PS 3901 High Impact Polystyrene Vystyrene PS 3901 is a black impact modified polystyrene compound with balanced impact/stiffness properties designed for injection molding applicationsFeatures: -High resilience -Excellent process.. |
|||
Middle Barrel Temperature | 185 °C | 365 °F | Compress zone |
Taiwan PU Corporation TPU-B90 General Grade, Blow Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Blow MoldingInformation provided by Taiwan PU Corporation. |
|||
Middle Barrel Temperature | 185 °C | 365 °F | Compress zone |
Taiwan PU Corporation TPU-BH90 Hydrolysis Resistance, Blow Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), Hydrolysis Resistance, Polyether Base, Blow MoldingInformation provided by Taiwan PU Corporation. |
|||
Middle Barrel Temperature | 185 °C | 365 °F | Compress zone |
Taiwan PU Corporation TPU-E85 General Grade, Extrusion Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Extrusion MoldingInformation provided by Taiwan PU Corporation. |
|||
Middle Barrel Temperature | 185 °C | 365 °F | Compress zone |
Taiwan PU Corporation TPUI-E90 General Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Middle Barrel Temperature | 185 °C | 365 °F | Compress zone |
Taiwan PU Corporation TPUI-G85 High Wear Resistance, Injection Molding Polycaprolactone Base TPU Thermoplastic Polyurethane (TPU), High Wear Resistance, Polycaprolactone Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Middle Barrel Temperature | 185 °C | 365 °F | Compress zone |
Taiwan PU Corporation TPUI-H90 High Hydrolysis Resistance, Injection Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Middle Barrel Temperature | 185 °C | 365 °F | Compress zone |
Taiwan PU Corporation TPUI-L85 Low Temperature Resistance, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), Low Temperature Resistance, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Middle Barrel Temperature | 185 - 195 °C | 365 - 383 °F | Transition, Extrusion |
Stellarchem DIOSHY® MP-960NC TPE Compound This grade of Stellarchem MP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, .. |
|||
Middle Barrel Temperature | 185 °C | 365 °F | |
SK Chemicals SKYTHANE® S175A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Middle Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8201-70 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Middle Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8221-70 Thermoplastic Elastomer A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Middle Barrel Temperature | 185 °C | 365 °F | Injection |
Alliance Polymers Viprene™ G70A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G70A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Middle Barrel Temperature | 185 °C | 365 °F | Injection |
Alliance Polymers Viprene™ G70A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G70A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Middle Barrel Temperature | 185 °C | 365 °F | Injection |
Alliance Polymers Viprene™ G75A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G75A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Middle Barrel Temperature | 185 °C | 365 °F | Injection |
Alliance Polymers Viprene™ G80A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G80A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Middle Barrel Temperature | 185 °C | 365 °F | Injection |
Alliance Polymers Viprene™ P75A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P75A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Middle Barrel Temperature | 185 °C | 365 °F | Injection |
Alliance Polymers Zythane™ 5070A Thermoplastic Polyurethane Elastomer Zythane™ 5070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Middle Barrel Temperature | 185 °C | 365 °F | Injection |
Alliance Polymers Viprene™ G85A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G85A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Middle Barrel Temperature | 185 °C | 365 °F | Injection |
Alliance Polymers Viprene™ P70A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P70A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Middle Barrel Temperature | 185 - 218 °C | 365 - 424 °F | |
Ineos Nova Zylar® 530 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:High clarityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specifications for Class VI plasticsUL94 HB @ 1.5 mm for uncolored ma.. |
|||
Middle Barrel Temperature | 185 - 218 °C | 365 - 424 °F | |
Ineos Nova Zylar® 631 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:Outstanding practical toughness and ductilityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationUSP Class VI compliantCustom colors and enhancement .. |
|||
Middle Barrel Temperature | 185 - 218 °C | 365 - 424 °F | |
Ineos Nova Zylar® 94-580-A High Performance Styrenic, Acrylic Copolymer
(discontinued **) Excellent heat distortion temperature, High clarity, strength and toughness, Enhanced mold releaseApplications: Industrial covers and housings, Paper towel dispenser covers, Appliance partsInjection.. |