Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 180 °C | 356 °F | Zone 1; Cylinder |
Premix Thermoplastics PRESEAL® TPE 6071 PRESEAL TPE 6071 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasketing and grounding applications. Conductivity is achieved with a silver coated glass sp.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | |
PTS POM-90 9.0 MFI Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 180 °C | 356 °F | Zone 2; Cylinder |
Premix Thermoplastics PRE-ELEC® CP 1315
(discontinued **) PRE-ELEC CP 1315 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical GPPS 20HR(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | |
LG Chemical LUCEL FW-710F Friction and Wear Resistant POM, PTEE filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | |
LG Chemical LUCEL FW-715C Friction and Wear Resistant POM, Polymeric Wear Additive, CaCo3 Filled, Low Warpage, Antistatic LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Middle Barrel Temperature | 180 - 230 °C | 356 - 446 °F | Injection |
Kolon DIAMAT® IG Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | |
LG Chemical LUCEL N109-02 General Purpose POM, Unreinforced, Externally Lubricated, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical LUCEL N109LDS POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | |
LG Chemical LUCEL N127-WR Weather Resistant POM, Unreinforced, High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | |
LG Chemical LUCEL N145-02 General Purpose POM, Unreinforced, Externally Lubricated, Ultra High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Middle Barrel Temperature | 180 - 190 °C | 356 - 374 °F | |
Huntsman AVALON® 75 AE Thermoplastic Polyurethane Introduction: AVALON 75 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 75 AE is part of the AVALON Soft Range and offers a premium soiling material .. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical 90HR SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Battery Case, Light CoverCAS No. 9003-54-7Information provided by LG Chemical |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
Stellarchem 475-860N TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
Stellarchem GP-860HD TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
Stellarchem MP-8001 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Middle Barrel Temperature | 180 - 220 °C | 356 - 428 °F | Injection |
Samyang Triel® 5400 Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r.. |
|||
Middle Barrel Temperature | >= 180 °C | >= 356 °F | |
Borealis Borcell™ LE1120 Low Density Polyethylene for Physically Foamed Cellular Insulation Borcell LE1120 is a low density polyethylene intended for the insulation of coaxial and radio frequency communication cables.. It contains no additives and is designed to give the lowest possible a.. |
|||
Middle Barrel Temperature | 180 - 220 °C | 356 - 428 °F | |
Borealis BS4641 High Density Polyethylene BS4641 is a bimodal high-density polyethylene homopolymer. Because of its excellent organoleptic properties, this grade is especially suitable for blow molding of bottles for food applications. App.. |
|||
Middle Barrel Temperature | 180 - 210 °C | 356 - 410 °F | |
Elastron® TPO Elastomer wide hardness rangedoes not require vulcanization-quite higher saving on the processing costsremains flexible at low temperatureshigh temperature resistanceelectrical insulator with very low conduct.. |
|||
Middle Barrel Temperature | 180 - 220 °C | 356 - 428 °F | Injection Molding |
LG Chemical KEYFLEX TO1075AR Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7 and 14807-96-6Information provided by LG Chemical |