Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 252 - 257 °C | 485 - 495 °F | |
Teknor Apex Chemlon® 240 MH Nylon 6, 40% Short Glass Fiber Reinforced Features: Heat Stabilized; Warp Resistant Forms: Pellets Additive: Heat Stabilizer Automotive Specifications: GM GMP.PA6.011Information Provided by Teknor Apex |
|||
Middle Barrel Temperature | 246 - 257 °C | 475 - 495 °F | |
Teknor Apex Chemlon® 225-15 MG Nylon 6, 25% Mineral Reinforced, 15% Glass Fiber Reinforced Features: Compound offering rigidity and strength, especially at high service temperatures; Excellent for large area parts Processing Method: Injection Molding Forms: Pellets Automotive Specificatio.. |
|||
Middle Barrel Temperature | 238 - 257 °C | 460 - 495 °F | |
Diamond Polymers ABS/PC FC-30 Description: Injection Molding Grade, High Impact, Flame RetardantInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 238 - 257 °C | 460 - 495 °F | |
Diamond Polymers ASA/PC FA-30 Description: ASA Weatherable Polymer, Injection Molding Grade, Flame RetardantInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 241 - 257 °C | 465 - 495 °F | |
Teknor Apex Chemlon® 214 GH Nylon 6, 14% Short Glass Fiber Features: Good Creep Resistance; Good Dimensional Stability; Good Processability; Good Toughness; Heat Stabilized; High Strength Processing Method: Injection Molding Forms: Pellets Additive: Heat S.. |