Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products F38-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Electrical housingsBracketsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products F43-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Fan shroudsDip trayFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products F43-01A 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Electrical component supportsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products M30P100-01 30% Mica Reinforced Polypropylene, Black Applications: Fan shroudsHVAC ductworkClose-out panelsFiller panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP 1049 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP 1093L Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP 1181 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1580B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1580L1-UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1625A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1657L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1695L1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1709C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1878B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1907E CLR Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2103 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2239 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2241 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP 1097F Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1351J Thermoplastic Elastomer Uses: Consumer Applications; Gaskets; Plumbing Parts; Pump Parts Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Drying is not necessary. However, if moisture is a p.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1366A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1380A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2840M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2850E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-4123 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2579B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2676B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products GC30P104-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: BracketsHead lamp housingsBattery trayInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP 1037 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2870E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |