Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT4700-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT4900-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Exterior componentsBodyside moldingsStep padsLicense plate bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT4900-33UV Thermoplastic Polyolefin, UV Stabilized, KSD Charcoal Argent Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT4900-74UV Thermoplastic Polyolefin, UV Stabilized, Exterior DX9 Black Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products G10P100-01UV 10% Glass Fiber Reinforced Polypropylene, UV Stabilized, Black Applications: BracketsIP structural componentsDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products G13P100-00 13% Glass Fiber Reinforced Polypropylene, Natural Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products G13P100-01UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, Black Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products G13P100-559UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM WPP 646H) Charcoal Metallic Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products GC10P250-00 10% Glass Fiber Reinforced Polypropylene Copolymer, Non-UV Stabilized, Chemically Coupled, Natural Applications: Component housingsStorage binsBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP514-199 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP514-393 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 110D Medium Dark Pewter Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP521-372 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 110D Medium Dark Pewter Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP522-00 15% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products T10P250-00 10% Talc Reinforced Polypropylene Copolymer, Natural Applications: Fan shroudsCenter consolesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products T10P250-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black Applications: Wire troughFan shroudsElectrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Polymer Resources ABS-GP1-[color]-3 ABS, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP520-00 12% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimCenter consolesGlove box binsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 227 °C | 399 - 441 °F | |
Ineos Nova 782 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, Custom colorsApplications: Multi-purpose injection molding where custom color is a requirement, Toys, Appliance, Computer peripheralsPerformance grades of polystyrene are engineered to ha.. |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/15/E Polypropylene Homopolymer, 15% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/30/E/M Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/30/E8/M Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® PP-60/TC/24/D/HS Polypropylene Homopolymer, Talc Filled, Heat Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® PP-60/TC/40 Polypropylene Homopolymer, 40% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® PP-61/CC/20 Polypropylene Copolymer, 20% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-62/30/E8 Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-68/10/E Polypropylene Copolymer, 10% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 399 - 441 °F | |
Ineos Nova 8047 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, Special additives can be incorporate to improve properties such as coefficient of friction and static dissipation, Custom colorsApplications: Injection molding, Designed for thin wall app.. |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-62/30/E Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products GC15P200-01 15% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Electrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |