Polymer Property : Middle Barrel Temperature = 171 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 171 - 188 °C
340 - 370 °F
PolyOne Dynaflex™ G2712-1000-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G2712-1000-02 is an easy processing TPE designed for injection molding and extrusion aplications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - High..
Middle Barrel Temperature 171 - 188 °C
340 - 370 °F
PolyOne Dynaflex™ G2780-0001 Thermoplastic Elastomer (TPE)
Dynaflex™ G2780-0001 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - Overmo..
Middle Barrel Temperature 171 - 193 °C
340 - 379 °F
PolyOne Dynalloy™ 8900-30 Thermoplastic Elastomer (TPE)
Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen..
Middle Barrel Temperature 171 - 193 °C
340 - 379 °F
PolyOne Dynalloy™ 8900-80 Thermoplastic Elastomer (TPE)
Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen..
Middle Barrel Temperature 171 - 188 °C
340 - 370 °F
PolyOne Dynaflex™ G2703-1000-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G2703-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance and a low coefficient of friction. - Adhesion to Polypropylen..
Middle Barrel Temperature 171 - 210 °C
340 - 410 °F
PolyOne Dynaflex™ G2706-1000-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G2706-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA and medical compliance. - High Puncture Reseal - Overmold Adhesion to Po..
Middle Barrel Temperature 171 - 188 °C
340 - 370 °F
PolyOne Dynaflex™ G2780C Thermoplastic Elastomer (TPE)
Dynaflex™ G2780C is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - Overmold A..
Middle Barrel Temperature 171 - 193 °C
340 - 379 °F
PolyOne Dynalloy™ 8900-60 Thermoplastic Elastomer (TPE)
Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen..
Middle Barrel Temperature 171 - 188 °C
340 - 370 °F
PolyOne Dynalloy™ OBC8200-BT50 Thermoplastic Elastomer (TPE)
Dynalloy™ OBC8200-BT50 is a translucent grade to be used in blow molding applications. New Product. Commercial specifications have not been established. - Excellent Colorability - Rubbery FeelPurge..
Middle Barrel Temperature 171 - 191 °C
340 - 375 °F
Ravago Manufacturing Americas Hylac® FR134G10 ABS, 10% Glass Fiber Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Middle Barrel Temperature 171 - 199 °C
340 - 390 °F
Ravago Manufacturing Americas Hylac® FR74 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Middle Barrel Temperature 171 - 182 °C
340 - 360 °F
Green Dot Terratek® BD 4015 Biodegradable Polymer
Terratek BD biodegradable composites are created from a proprietary blend of starch-based ingredients and other materials, the natural components derived from renewable grain sources account for the..
Middle Barrel Temperature 171 - 188 °C
340 - 370 °F
Teknor Apex Flexalloy® 9100-55 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather..
Middle Barrel Temperature 171 - 193 °C
340 - 380 °F
Tempia Polylactic acid (PLA) Resin
A bio-degradable plastic, Polylactic acid (PLA) is made from corn. Products produced are compostable within 45 – 120 days. The degradation process of the item is temperature, humidity and thicknes..
Middle Barrel Temperature >= 171 °C
>= 340 °F
Borealis Visico™ LE4421/LE4432 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation
LE4421/LE4432 is a black, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination of a VISICO™ base material, LE4..
Middle Barrel Temperature >= 171 °C
>= 340 °F
Borealis Visico™ LE4421/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation
Visico LE4421/LE4437 is a natural, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination of a Visico base materi..
Middle Barrel Temperature >= 171 °C
>= 340 °F
Borealis Visico™ LE4421/LE4460/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation
Visico LE4421/LE4460/LE4437 is a natural, halogen-based, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination o..
Middle Barrel Temperature >= 171 °C
>= 340 °F
Borealis Visico™ LE4423/LE4432 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation
Visico LE4423/LE4432 is a black, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination of a Visico base material..
Middle Barrel Temperature >= 171 °C
>= 340 °F
Borealis Visico™ LE4423/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation
Visico LE4423/LE4437 is a mature, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination of a Visico base materia..
Middle Barrel Temperature >= 171 °C
>= 340 °F
Borealis Visico™ LE4421/LE4460/LE4432 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation
Visico LE4421/LE4460/LE4432 is a black, halogen-based flame retardant, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The..
Middle Barrel Temperature 171 - 195 °C
340 - 383 °F
A. Schulman ComAlloy Voloy® 101 Polypropylene, Impact Modified, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.