Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 180 - 200 °C | 356 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-0837 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Zone 3 | 180 - 200 °C | 356 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-7666/GY Polyacetal-copolymer, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Zone 3 | 180 - 200 °C | 356 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-7727 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Zone 3 | 180 - 200 °C | 356 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-8268 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Zone 3 | 180 - 200 °C | 356 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-8444 Polyacetal-copolymer, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.dynamic stressReduced moment of inertia compared with metal parts.Isotropic shrinkage character.. |
|||
Zone 3 | 180 - 200 °C | 356 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-8510 Polyacetal-copolymer, with mineral filler, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Zone 3 | 180 - 200 °C | 356 - 392 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 10288D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 3 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/2 Polyolefin Catalyst PS/2 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that take place by exposure of the pipe to water or steam .. |
|||
Zone 3 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/2 UV Polyolefin Catalyst PS/2 UV is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or.. |
|||
Zone 3 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® PNT 0553/23 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0553/23 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo.. |
|||
Zone 3 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® T/A-LX Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LX is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Zone 3 | 190 - 200 °C | 374 - 392 °F | Injection |
Lubrizol ESTANE® GP80AB Ester Based Thermoplastic Polyurethane Type: Estane® GP 80AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Zone 3 | 190 - 200 °C | 374 - 392 °F | |
Eurostar Starflam MX05036 PP, Flame Retardant, Injection Molding Starflam MX05036 is an Unfilled, Halogen Free Flame Retardant, Polypropylene Injection Molding ResinInformation provided by Eurostar. |