Processing Properties Metric English Comments
Zone 3 220 °C
428 °F
Die
Premix Thermoplastics PRE-ELEC® PE 1296 Conductive Thermoplastic Compound
PRE-ELEC® PE 1296 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1296 has a high concentration o..
Zone 3 220 °C
428 °F
Cylinder
Premix Thermoplastics PRE-ELEC® PE 1296 Conductive Thermoplastic Compound
PRE-ELEC® PE 1296 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1296 has a high concentration o..
Zone 3 220 °C
428 °F
Die
Premix Thermoplastics PRE-ELEC® PP 1391 Conductive Thermoplastic Compound
PRE-ELEC® PP 1391 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Zone 3 220 - 240 °C
428 - 464 °F
Extrusion
Kolon DIAMAT® EM
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Zone 3 220 - 240 °C
428 - 464 °F
Extrusion
Kolon DIAMAT® IH
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Zone 3 220 - 240 °C
428 - 464 °F
Extrusion Molding
LG Chemical LUPOL GP1007FE Flame Retardant PP
Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical
Zone 3 220 - 230 °C
428 - 446 °F
Lubrizol Advanced Materials Pearlthane® 12H92E Thermoplastic Polyurethane Elastomer
Pearlthane® 12H92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and excellent low temperature performance..
Zone 3 220 - 230 °C
428 - 446 °F
Lubrizol Advanced Materials Pearlthane® ECO D12T90E Thermoplastic Polyurethane
PEARLTHANE® ECO D12T90E is a 91 Shore A, High Performance natural TPU based on Renewable Sources with ca. 37% renewable content according to ASTM D6866 for Extrusion and Blow moulding application..
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3020IX1 Rigid Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: conductive, impact modifiedInformation provided by UBE.
Zone 3 220 °C
428 °F
Injection Molding
UBE UBESTA® 3024NUX Short Cycle Time Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030JI5L 8x1 mm Black Automotive Grade Nylon 12 Tube
Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, impact modified and stabilized against weatherability (DIN 73378 Nomenclature = PA12 HIPHL)Information provided by U..
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030JLX1 8x1 mm Black Automotive Grade Nylon 12 Tube
Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, stabilized against weatherability (DIN 73378 Nomenclature = PA12 PHL)Information provided by UBE.
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Ethanol for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Formic Acid (10%) for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Hydrochloric Acid (10%) for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Water for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030JLX2 Plasticized Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: semi-plasticized, UV resistance, heat resistanceInformation provided by UBE.
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Calcium Chloride aq. for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Methanol for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Sodium Hydroide for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Xylene for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Zinc chloride aq. for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3035LU1 Rigid Piping Grade Nylon 12
Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron..
Zone 3 220 - 300 °C
428 - 572 °F
Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Dry, 30% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Sodium Hydroide for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..