Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 215 - 235 °C | 419 - 455 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1155D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 3 | 215 - 235 °C | 419 - 455 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 3038D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 3 | 215 - 235 °C | 419 - 455 °F | Extrusion Molding |
LG Chemical KEYFLEX BT GN7155F Ester Type TPE Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical |
|||
Zone 3 | 215 - 225 °C | 419 - 437 °F | |
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer Type: Pearlthane® 11H98 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining a unique set of properties such as mec.. |
|||
Zone 3 | 215 °C | 419 °F | |
Lubrizol Advanced Materials Pearlthane® D16N60D Thermoplastic Polyurethane Elastomer Type : Pearlthane® 16N60D is a polyether-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining high hardness with excellent mechanical properties and .. |
|||
Zone 3 | 215 °C | 419 °F | |
Borealis Borcell™ HE4873 High Density Polyethylene Borcell™ HE4873 is a fully formulated compound for physical foamed data cable insulation. Borcell™ HE4873 is a high-density polyethylene compound containing blowing agent for the production of foa.. |
|||
Zone 3 | 215 - 225 °C | 419 - 437 °F | Extrusion |
Lubrizol Isoplast® 300 Engineering Thermoplastic Polyurethane Resin Type: Isoplast® 300 is an engineering thermoplastic polyurethane resin.Appearance: Clear transparent pelletsApplication: Sheet extrusion, composite structures for industrial and consumer goods, inj.. |
|||
Zone 3 | 215 - 225 °C | 419 - 437 °F | Injection |
Lubrizol ESTANE® GP60DB Ester Based Thermoplastic Polyurethane Type: Estane® GP 60DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tags.Available in.. |
|||
Zone 3 | 215 - 225 °C | 419 - 437 °F | Injection |
Lubrizol ESTANE® GP72DB Ester Based Thermoplastic Polyurethane Type: Estane® GP 72DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, TranslucentAvailable in EuropeInformati.. |
|||
Zone 3 | 215 °C | 419 °F | Extrusion |
Alliance Polymers Zythane™ 5050D Thermoplastic Polyurethane Elastomer Zythane™ 5050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Zone 3 | 215 °C | 419 °F | Extrusion |
Alliance Polymers Zythane™ 7050D Thermoplastic Polyurethane Elastomer Zythane™ 7050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |