Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 230 - 260 °C | 446 - 500 °F | hopper |
Nilit Nilamid B3N Unfilled, Nucleated PA6 Description: Nilamid B3N is an unfilled, nucleated NYLON 6. It is fast cycling, and combines ease of processing with good overall mechanical characteristics.Key characteristics: Fast cyclingEasy pro.. |
|||
Zone 1 | 230 - 260 °C | 446 - 500 °F | hopper |
Nilit Nilamid B3 H ZB Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZB is a high impact NYLON 6. The product has excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas inclu.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/13/SI/2 PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7692/BK PBT, with glass spheres and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7783 PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7783-1 PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7853 PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7942/RD PBT, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7952 PBT, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-8322 PBT, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850/PL/15/BK PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Parts for electric and electro.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7557 PBT, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour, self-lubricating, for highest tribologic needs.Low warpag.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7581 PBT, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Zone 1 | 220 - 260 °C | 428 - 500 °F | |
Lehmann & Voss LUVOCOM® NY-4/PL/15/BK Polyamide 612, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Zone 1 | 230 - 260 °C | 446 - 500 °F | |
Topas Advanced Polymers TOPAS® 5013L-10 Cyclic Olefin Copolymer (COC) TOPAS® 5013L-10 is a high flow, internally lubricated injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, che.. |
|||
Zone 1 | 250 - 260 °C | 482 - 500 °F | |
Eurostar Staramide PB00A PA6, 50% Glass Bead Filled, Injection Molded Staramide PB00A is a 50% Glass Bead Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |