Processing Properties Metric English Comments
Zone 1 335 - 390 °C
635 - 734 °F
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU)  (Unverified Data**)
Veradel A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to st..
Zone 1 370 - 390 °C
698 - 734 °F
Lehmann & Voss LUVOCOM® 1115/XCF/40 PEK, with carbon fiber
Applications: High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts, non flammable.Electrically c..
Zone 1 370 - 390 °C
698 - 734 °F
Lehmann & Voss LUVOCOM® PEKK-7299 Polyether ketone, with carbon fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Suitable for discharging of statically generated electricity.Thermic,..
Zone 1 370 - 390 °C
698 - 734 °F
Lehmann & Voss LUVOCOM® TPI-0953 Thermoplastic polyimide, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, apparatus- and precision engineering medical- and electrical enineering, aircraft- and aerospace industry.Very high continuous use and heat dist..
Zone 1 370 - 390 °C
698 - 734 °F
Lehmann & Voss LUVOCOM® TPI-8257 Thermoplastic polyimide, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering medical- and electrical enineering, aircraft- and aerospace industry.High-strength and high-stiff parts; lo..
Zone 1 370 - 390 °C
698 - 734 °F
Lehmann & Voss LUVOCOM® 1104/XCF/30 Polyether ketone, with carbon fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Suitable for discharging of statically generated electricity.Thermic,..
Zone 1 370 - 390 °C
698 - 734 °F
Lehmann & Voss LUVOCOM® 1104-7452 Polyether ketone, with glass fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Improved fatigue properties.Thermic, mechanic and chemical highly str..
Zone 1 370 - 390 °C
698 - 734 °F
Lehmann & Voss LUVOCOM® 1104-7598 Polyether ketone, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Improved fatigue properties.Thermic, mechanic and chemical highly str..
Zone 1 370 - 390 °C
698 - 734 °F
Lehmann & Voss LUVOCOM® 1104-7824 Polyether ketone, with carbon fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Suitable for discharging of statically generated electricity.Thermic,..
Zone 1 370 - 390 °C
698 - 734 °F
Lehmann & Voss LUVOCOM® 1104-8327 Polyether ketone, with glass fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts.Low warpage.Information pro..
Zone 1 335 - 390 °C
635 - 734 °F
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU)
Veradel® A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance t..