Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 160 °C | 320 °F | |
DuPont Nucrel® 535 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 535 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Zone 1 | 160 °C | 320 °F | |
DuPont Nucrel® 2940 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2940is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Zone 1 | 160 °C | 320 °F | |
Termopol Termoton® K2GA4065A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Zone 1 | 160 °C | 320 °F | |
Termopol Termoton® K2GA5080A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Zone 1 | 160 °C | 320 °F | |
Termopol Termoton® V2GA0065A TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
Zone 1 | 160 °C | 320 °F | |
Termopol Termoton® V2GA1065A TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
Zone 1 | 160 °C | 320 °F | |
DuPont Nucrel® 2806 Ethylene-Acrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2806 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for.. |
|||
Zone 1 | 160 - 200 °C | 320 - 392 °F | |
Lehmann & Voss LUVOCOM® 94-8485 LD-PE, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Reduced moment of inertia compared with metal parts.Dynamic stressed parts.Especially suitable .. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Extrusion Molding |
Kolon ELLAS K-260D Thermoplastic Polyurethane ApplicationsExtrusion: Antenna, Heel TipInjection: Hose, Tube, SheetIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Injection Molding |
Kolon ELLAS K-296AB Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Pneumatic tube, film/sheet, cableTransparent HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Injection Molding |
Kolon ELLAS K-395A Ether Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Cable sheathing, Highly Pressurized HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Extrusion Molding |
Kolon ELLAS K-395A Ether Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Cable sheathing, Highly Pressurized HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Injection Molding |
Kolon ELLAS K-470A Ester Based Thermoplastic Polyurethane ApplicationsInjectionIndustry PartsParts for Automobile/Mobile phoneABS Compound |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Injection Molding |
Kolon ELLAS K-585A Caprolactone Based Thermoplastic Polyurethane ApplicationsInjectionIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Extrusion Molding |
Kolon ELLAS K-793AB Ester Based Thermoplastic Polyurethane ApplicationsFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Extrusion Molding |
Kolon ELLAS K-796A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionPneumatic HoseTransparent HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 160 - 168 °C | 320 - 335 °F | |
Lubrizol Advanced Materials PEARLCOAT® 162K Thermoplastic Polyurethane Elastomer PEARLCOAT® 162K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and very good hydrolysis resistance. PE.. |
|||
Zone 1 | 160 - 170 °C | 320 - 338 °F | |
Silon Taborex TA 1117HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1117 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Zone 1 | 160 - 170 °C | 320 - 338 °F | |
Silon Taborex TA 1133 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1133 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Zone 1 | 160 - 170 °C | 320 - 338 °F | |
Silon Taborex TA 1108 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1108 HD is a crosslinkable compound according to the “SIOPLAS-SYSTEMâ€; made by a Silane grafted ethylene copolymer known as the graft and a Masterbatch containing the crosslinki.. |
|||
Zone 1 | 160 °C | 320 °F | Extrusion |
Lubrizol Estane® ZHF 82AT0 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 82AT0 NAT021 is an 82A aromatic polyether-based, non-halogen flame retardant, thermoplastic polyurethane (TPU) compound.Features: Soft, matte finished, good flame retardant proper.. |
|||
Zone 1 | 160 °C | 320 °F | Extrusion |
Lubrizol Estane® ZHF 95AT3 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 95AT3 TPU is a zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding flame retardant properties, especially suited for tray cables.. |
|||
Zone 1 | 160 °C | 320 °F | |
Borealis Casico™ FR6082 Reduced Fire Hazard Jacketing Compound Casico™ FR6082 is a thermoplastic, reduced fire hazard, zero halogen black jacketing compound combined with high mechanical strength, toughness and excellent extrusion properties. It is based on th.. |
|||
Zone 1 | 160 °C | 320 °F | |
Borealis FL5580 High Density Polyethylene FL5580 is a high density polyethylene with an excellent combination of extrusion properties and moisture barrier properties. Applications: FL5580 has been developed especially for applications like.. |
|||
Zone 1 | 160 °C | 320 °F | |
DuPont Nucrel® 925 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 925 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Zone 1 | 160 °C | 320 °F | |
DuPont Nucrel® 599 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Zone 1 | 160 - 180 °C | 320 - 356 °F | |
Arkema Group OREVAC® 18365-S Grafted Maleic Anhydride Polyethylene OREVAC 18365-S is a grafted maleic anhydride polyethylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC 18365-S is mainly used in multi-layer tube to have good adhesion between.. |
|||
Zone 1 | 160 - 180 °C | 320 - 356 °F | |
Arkema Group OREVAC® 18510 Grafted Maleic Anhydride Polyethylene OREVAC 18510 is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE or HDPE coating for steel pipeline. It is a powder product. OREVAC 18510 is mainly used in pipe .. |
|||
Zone 1 | 160 °C | 320 °F | |
Termopol Termoton® K2GA2060A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |