Polymer Property : Adapter Temperature = 455 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Adapter Temperature 235 - 245 °C
455 - 473 °F
Average value: 240 °C Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
Adapter Temperature 235 °C
455 °F
For coextrusion with EVA or EVOH.
DuPont Bynel® 41E623 Adhesive Resin  (discontinued **)
Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design..
Adapter Temperature 235 - 245 °C
455 - 473 °F
LG Chemical AT-553 Transparent ABS, Permanent Antistatic, Natural and Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
Adapter Temperature 235 - 245 °C
455 - 473 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1072D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Adapter Temperature 235 - 245 °C
455 - 473 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1172D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical
Adapter Temperature 235 - 245 °C
455 - 473 °F
LG Chemical TR-557I Transparent ABS, High Impact, Ice Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
Adapter Temperature 235 - 245 °C
455 - 473 °F
LG Chemical TR-558AI Transparent ABS, High Stiffness, Ice Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
Adapter Temperature 235 - 245 °C
455 - 473 °F
LG Chemical TR-558NS Transparent ABS, Antistatic, Natural and Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
Adapter Temperature 235 °C
455 °F
DuPont Bynel® 3126 Adhesive Resin
Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce..
Adapter Temperature 235 °C
455 °F
DuPont Bynel® 39E660 Adhesive Resin
Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Adapter Temperature 235 °C
455 °F
For coextrusion with EVA or EVOH.
DuPont Bynel® 42E703 Adhesive Resin
Bynel® Series 4200 resins are anhydride-modified low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Adapter Temperature 235 °C
455 °F
DuPont Bynel® 30E670 Adhesive Resin
Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Adapter Temperature 235 °C
455 °F
Extrusion Coating
DuPont™ Appeel® 20D828 Ethylene Acrylate
Appeel® 20D828 is an modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad temp..
Adapter Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 21E533 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i..
Adapter Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 21E787 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i..
Adapter Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 21E810 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester that allows them to be functional in high temperature coextrusions. They are avail..
Adapter Temperature 235 °C
455 °F
Cast Film/Sheet Processing
DuPont™ Bynel® 22E780 Modified Ethylene Acrylate
BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f..
Adapter Temperature 235 °C
455 °F
Extrusion Coating
DuPont™ Bynel® 30E783 Anhydride Modified Ethylene Vinyl Acetate
BYNEL® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Adapter Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 41E710 Anhydride Modified LLDPE
BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi..
Adapter Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 41E850 Anhydride Modified LLDPE
BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext..
Adapter Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 41E871 Anhydride Modified LLDPE
BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext..
Adapter Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 50E662 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
Adapter Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 50E725 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
Adapter Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 50E739 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
Adapter Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 50E806 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
Adapter Temperature 235 °C
455 °F
Extrusion Coating
DuPont™ Elvaloy® AC 12024S Ethylene Methyl Acrylate
Elvaloy® AC 12024S is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy®..
Adapter Temperature 235 °C
455 °F
Cast Film/Sheet Processing
DuPont™ Surlyn® 1706 Zinc Ionomer
Surlyn® 1706 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t..
Adapter Temperature 235 °C
455 °F
Cast Film/Sheet Processing
DuPont™ Surlyn® 1707 Sodium Ionomer
Surlyn® 1707 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t..
Adapter Temperature 235 °C
455 °F
Cast Film/Sheet Processing
DuPont™ Surlyn® 2601B Sodium Ionomer
Surlyn® 2601B is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer ..
Adapter Temperature 235 °C
455 °F
For coextrusion with EVA or EVOH.
DuPont Bynel® 50E662 Adhesive Resin  (discontinued **)
Bynel® Series 5000 resins are anhydride-modified polypropylene. Bynel® 50E662 are based on polypropylene random copolymers. They are available in pellet form for use in conventional extrusion an..