Processing Properties | Metric | English | Comments |
---|---|---|---|
Feed Temperature | 60.0 - 75.0 °C | 140 - 167 °F | Injection molding |
Hexion Bakelite™ PF 13 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically mica filled, heat resistance, good electrical properties, UL listed molding compound 0.75 mm/V-1 (NC), 3 mm/V-0, standardized molding compound.Application ar.. |
|||
Feed Temperature | 60.0 - 75.0 °C | 140 - 167 °F | Injection molding |
Hexion Bakelite™ PF 51 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Contact support power switch, switch.. |
|||
Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Tisan TISLAMID® 6 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
Eurotec® Tecomid® NA40 GR40 NL HS PA6.6, 40% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
Eurotec® Tecomid® NA40 GR40 NL RM PA6.6, 40% glass fiber reinforced, MoS2 modified, natural Information provided by Eurotec® |
|||
Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
Eurotec® Tecomid® NA40 MR15 NL IL PA6.6, 15% mineral filled, impact modified, natural Information provided by Eurotec® |
|||
Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
Eurotec® Tecomid® NB30 GR15 BK005 FS90 PA6, 15% glass fiber reinforced, flame retardant - halogen & red phosphorus free, low smoke & toxic gas grade Information provided by Eurotec® |
|||
Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
Eurotec® Tecomid® NB40 GB30 NL PA6, 30% glass bead reinforced, natural Information provided by Eurotec® |
|||
Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
Eurotec® Tecomid® NB40 NL IL PA6, impact modified, natural Information provided by Eurotec® |
|||
Feed Temperature | <= 60.0 °C | <= 140 °F | Throat |
Eurotec® Tecolen® CP20 GB30 NL PPCP, 30% glass bead reinforced, natural Information provided by Eurotec® |
|||
Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
Eurotec® Tecotek® PC43 GR003 TD70 PC, unfilled, flame retardant - halogen (RoHS compliant), impact modified, light grey Information provided by Eurotec® |
|||
Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Akro-Plastic Akromid® B3 GF 50 RM-M (3146) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Akro-Plastic Akromid® B3 GF 60 (2476) PA 6 Dry, 60% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Akro-Plastic Akromid® A3 GF 15 (2418) PA 6.6 Dry, 15% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Akro-Plastic Akromid® B3 GF 10 (2829) PA 6 Dry, 10% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Akro-Plastic Akromid® S3 GF 50 1 (3533) PA 6.10 Dry, 50% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
Eurotec® Tecomid® NB40 NL IH PA6, impact modified, natural Information provided by Eurotec® |
|||
Feed Temperature | 60.0 - 75.0 °C | 140 - 167 °F | Injection molding |
Hexion Bakelite™ EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage Epoxy molding compound, inorganically filled, glass fiber reinforced, heat resistant, dimensionally stable, good electrical and mechanical properties, very good chemical resistance, low viscosity, U.. |