Polymer Property : Drying Temperature = 100 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5 BK PPS, linear, with carbon fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301/GF/30/TF/15 PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-7153 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. ..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-7293/GN PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-7661/RD PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-7662/BK PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-7836 PPS, linear, with glass fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Low warpage, isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts.High dim..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-8077 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricity.S..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-8306 PPS, linear, with carbon fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Improved friction and wear behaviour. Emergency running property.Inherent flam..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-8349 PPS, linear, with PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinkage ..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-8367 PPS, linear, with CNT
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. ..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-8386 PPS, linear, with aramid reinforcement and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-8400 PPS, linear, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Improved friction and wear behaviour. Emergency runni..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-8517 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-8524 PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-7575 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-7629/EG PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-8060 PPS, linear, with glass fiber and PTFE, high viscosity
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Low warpage, isotropic shrinkage characteristics.Improved friction and wear be..
Drying Temperature 100 °C

@Time 14400 sec
212 °F

@Time 4.00 hour
Chute Hot-Wind
Zhejiang Juner PC/ABS Alloy
Applications: Shell of Small Household Electric ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd.
Drying Temperature 100 °C

@Time 18000 sec
212 °F

@Time 5.00 hour
Chute Hot-Wind
Zhejiang Juner PC/PBT Alloy
Applications: Shell of Small Household Electric Appliance, Auto Electric Appliance PartsInformation provided by Zhejiang Juner New Materials Co, Ltd.
Drying Temperature 100 °C

@Time 18000 sec
212 °F

@Time 5.00 hour
Chute Hot-Wind
Zhejiang Juner PC/PET Alloy
Applications: Shell of Small Household Electric Appliance, Auto Electric Appliance PartsInformation provided by Zhejiang Juner New Materials Co, Ltd.
Drying Temperature 100 °C

@Time 28800 sec
212 °F

@Time 8.00 hour
Horizontal Oven
Zhejiang Juner PC/PET Alloy
Applications: Shell of Small Household Electric Appliance, Auto Electric Appliance PartsInformation provided by Zhejiang Juner New Materials Co, Ltd.
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301/CF/10/GF/20/GK/20/BK100 PPS, linear, with carbon fiber, glass fiber and micro glass spheres
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-8212/BL PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr..
Drying Temperature 100 °C

@Time 14400 sec
212 °F

@Time 4.00 hour
Chute Hot-Wind
Zhejiang Juner PC/ABSz-4 Alloy
Applications: Shell of Small Household Electric ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd.
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-8291 PPS, linear, with aramid reinforcement
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma..
Copyright © lookpolymers.com All Rights Reserved