Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | |
Resin Technology Group 1105 Oxy-Bond™ Two-Component Epoxy Adhesive Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma.. |
|||
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | |
Resin Technology Group 1105 Oxy-Bond™ Two-Component Epoxy Adhesive Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma.. |
|||
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | Small Mass |
Resin Technology Group TIGA 101-EX Five-Minute Epoxy Adhesive 1 part resin to 1 part hardener.TIGA 101-EX is an exceptional epoxy formulation, recommended for lower temperature or wet industrial bonding applications where fast curing is required. This clear, t.. |
|||
Pot Life | 4.0 - 5.0 min | 4.0 - 5.0 min | Time before parts must be mated |
Lord Adhesives 7542B Two-Component Urethane Adhesive Lord Urethane AdhesivesLord® one- and two-part urethane adhesives provide superior bonds with minimal surface preparation for today's high performance thermosets and thermoplastics. They offe.. |
|||
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | Time before parts must be mated |
Lord Adhesives 7545B Two-Component, Equal-Mix, Non-Sag Urethane Adhesive Lord Urethane AdhesivesLord® one- and two-part urethane adhesives provide superior bonds with minimal surface preparation for today's high performance thermosets and thermoplastics. They offe.. |
|||
Pot Life | 4.0 - 5.0 min @Temperature 25.0 °C |
4.0 - 5.0 min @Temperature 77.0 °F |
|
Lord Adhesives Thermoset™ UR-322 Two Component Urethane Potting Compound Lord UR-322 is a two component, room temperature curing urethane potting compound. The cured elastomer is soft, flexible and has a very low modulus at temperatures down to -80°C. Cured UR-322 als.. |
|||
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | 100 gram mass |
Master Bond EP21LVSP6 Two component epoxy for bonding, sealing, coating and encapsulating Product Description: Master Bond EP21LVSP6 is a two component epoxy compound for high performance bonding, coating, sealing and encapsulating. It is formulated to cure at room temperature or more ra.. |
|||
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | Mass: 25g; TM R050-19 |
Resinlab® EP1026 Clear Epoxy Adhesive Resinlab™ EP1026 Clear is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in .. |
|||
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | Mass: 50g; TM R050-19 |
Resinlab® EP1026HP Epoxy Adhesive Resinlab™ EP1026HP is a high performance fast setting epoxy adhesive designed for bonding metals, ceramics, glass and most plastics. This product gives good resistance to water salt spray, inorgan.. |
|||
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | Mass: 50g; TM R050-19 |
Resinlab® EP1026R Rubber Modified Epoxy Adhesive Resinlab™ EP1026R is a two part unfilled rubber modified epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free .. |
|||
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | |
Loctite® Durabond® E-00CL Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | |
Loctite® Durabond® E-00NS Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | |
Loctite® Durabond® E-05CL Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | Mass: 25g; TM R050-19 |
Resinlab® EP1026 Black Epoxy Adhesive Resinlab™ EP1026 Black is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in .. |