Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 90 - 120 min | 90 - 120 min | Mass: 100g; TM R050-19 |
Resinlab® EP1121-4 Adhesive / Casting Resin Resinlab™ EP1121-4 is a highly filled, high viscosity black adhesive / casting resin designed for applications requiring a high degree of thermal conductivity, flexibility, and a low CTE. It gives .. |
|||
Pot Life | 60 - 120 min | 60 - 120 min | |
NextGen Adhesives P907-12 Fiber Optic Adhesive Description: NGAC P907-12 is a rapid curing, low viscosity, heat cured epoxy adhesive system that is specifically formulated for use in the fiber optic industry.Advantages and Applications: Uses inc.. |
|||
Pot Life | 60 - 120 min | 60 - 120 min | |
NextGen Adhesives P907-13 Fiber Optic Adhesive Description: NGAC P907-13 is a rapid curing, low viscosity, heat cured epoxy adhesive system that is specifically formulated for use in the fiber optic industry.Advantages and Applications: Uses inc.. |
|||
Pot Life | 60.0 - 120 min @Temperature 20.0 °C |
60.0 - 120 min @Temperature 68.0 °F |
|
Permabond ET505 Epoxy Resin PERMABOND ET505 is a two-part, 1:1 mixable epoxy adhesive. ET505 is a semi-flexible toughened epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plas.. |
|||
Pot Life | 60 - 120 min | 60 - 120 min | Mass: 100g |
Resinlab® EP324E Clear Two Part Epoxy Casting Resin Resinlab™ EP 324E Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wettin.. |
|||
Pot Life | 120 - 120 min @Temperature 80.0 - 80.0 °C |
120 - 120 min @Temperature 176 - 176 °F |
Average value: 120 min Grade Count:1 |
Overview of materials for Epoxy, High Temperature This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val.. |
|||
Pot Life | 90 - 120 min | 90 - 120 min | Time before parts must be mated |
Lord Adhesives 309 General Purpose, Non-Sag, Thixotropic Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Pot Life | 90 - 120 min | 90 - 120 min | Curing |
Silikony Polskie Gumosil M Silicone Rubber Flexible with good tearing resistance |
|||
Pot Life | 90 - 120 min | 90 - 120 min | 100 gram mass |
Master Bond EP21AOLV-1 Two Part, Room Temperature Curing Epoxy System Product Description: Master Bond Polymer Adhesive EP21AOLV-1 is a two component, thermally conductive, electrically isolating epoxy adhesive, sealant and coating. This versatile system will adhere t.. |
|||
Pot Life | 90 - 120 min | 90 - 120 min | 100 gram mass |
Master Bond EP21NDLO Low Outgassing, Room Temperature Curing Two Component Epoxy Master Bond EP21ND-LO is a two component, room temperature curing epoxy system for bonding, sealing and coating featuring outstanding physical properties. EP21ND-LO has a convenient one to one mix r.. |
|||
Pot Life | 90 - 120 min | 90 - 120 min | 100 gram mass |
Master Bond EP21TDCHT-LO Room Temperature Curing, Toughened Two Component Epoxy Master Bond Polymer Adhesive EP21TDCHT-LO is a two component epoxy adhesive formulated to cure at room temperature or more rapidly at elevated temperatures, with a very forgiving and convenient one .. |
|||
Pot Life | 90 - 120 min | 90 - 120 min | 100 gram mass |
Master Bond EP21TDCHTND Versatile, toughened two component epoxy for bonding, sealing and coating Product Description: Master Bond EP21TDCHTND is a two component epoxy adhesive, sealant and coating featuring high performance, versatility and exceptional user friendliness. It has a very forgiving.. |
|||
Pot Life | 90 - 120 min | 90 - 120 min | 100 gram mass |
Master Bond EP21TPFL-1AO Two Part, Flexible, Lower Viscosity Epoxy Polysulfide System Product Description: Master Bond EP21TPFL-1AO is a two component, low viscosity epoxy polysulfide for high performance bonding, sealing, coating and casting offering thermal conductivity, electrical.. |
|||
Pot Life | 75 - 120 min | 75 - 120 min | 100 gram batch |
Master Bond EP33ND Epoxy Paste Resists Harsh Chemicals Description: Master Bond EP33ND is a two part, room temperature curing epoxy system used for bonding, sealing and coating featuring high temperature resistance, good dimensional stability and very g.. |
|||
Pot Life | 100 - 120 min | 100 - 120 min | 100 gram mass |
Master Bond EP40 High Shear and Peel Strength, Two Component, Flexible Epoxy Master Bond Polymer System EP40 is newly developed two component highly flexible epoxy compound for high performance bonding, potting, encapsulation, and sealing with outstanding shear and peel stre.. |
|||
Pot Life | 90.0 - 120 min @Temperature 25.0 °C |
90.0 - 120 min @Temperature 77.0 °F |
100 grams |
Cytec (Conap) FR-1273 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Pot Life | 60 - 120 min | 60 - 120 min | |
Epoxy Technology EPO-TEK® 301 Spectrally Transparent Epoxy Product Description: EPO-TEK® 301 is a two component, room temperature curing epoxy featuring very low viscosity, and excellent optical-mechanical properties.Advantages & Application Notes: Semicon.. |
|||
Pot Life | 60.0 - 120 min | 60.0 - 120 min | |
Aremco Ceramacast™ 575-N High Temperature Potting & Casting Material Alumina Fine grain castable for potting and producing small tools. |
|||
Pot Life | 60 - 120 min | 60 - 120 min | |
Aremco Ceramacast™ 576-N High Temperature Potting & Casting Alumina Medium grain castable ceramic for large high temperature potting and tooling. Aremco offers a range of ceramic-based materials used for the assembly of high temperature, high power electrical devic.. |
|||
Pot Life | 60 - 120 min | 60 - 120 min | |
Aremco Ceramacast™ 586 High Temperature Potting & Casting Material Zirconia Silicate Castable ceramic for ceramic and metal assemblies. Excellent handling, fast curing. |
|||
Pot Life | 60 - 120 min | 60 - 120 min | |
Aremco Ceramacast™ 646-N High Temperature Potting & Casting Material Zirconia Castable ceramic with high dielectric and physical strength. |
|||
Pot Life | 60 - 120 min | 60 - 120 min | |
Aremco Ceramacast™ 675 High Temperature Potting & Casting Material Aluminum Nitride Fine grain aluminum nitride castable with high thermal conductivity |
|||
Pot Life | 80 - 120 min | 80 - 120 min | |
Abatron AboCast 7703-21/AboCure 7703-21 (A) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Pot Life | 80 - 120 min | 80 - 120 min | |
Abatron AboCast 7703-21/AboCure 7703-23 (C) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Pot Life | 80 - 120 min | 80 - 120 min | |
Abatron AboCast 7703-21/AboCure 7703-24 (D) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Pot Life | 90 - 120 min | 90 - 120 min | Mass: 100g; TM R050-19 |
Resinlab® EP1282 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1282 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It is recognized under the Component Recognition Program of Underwriters Laborat.. |
|||
Pot Life | 90 - 120 min | 90 - 120 min | Mass: 100g; TM R050-19 |
Resinlab® EP1282 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1282 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It is recognized under the Component Recognition Program of Underwriters Laborat.. |
|||
Pot Life | 2.00 - 120 min | 2.00 - 120 min | Average value: 28.2 min Grade Count:21 |
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and .. |