Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 204 - 218 °C | 400 - 425 °F | Suggested Stock |
S&E Specialty Polymers TufGuard M™ GPP1005M-CD PP, Flame Retardant Application: A UL94 V-2, flame retardant polypropylene compound for injection molding applications, including cases for industrial power supply. Compound is designed with halogen-based flame retarda.. |
|||
Processing Temperature | 204 - 238 °C | 400 - 460 °F | Average value: 221 °C Grade Count:6 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Processing Temperature | 204 - 227 °C | 400 - 440 °F | Injection |
Shuman 710H Utility Black ABS Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc. |
|||
Processing Temperature | 204 - 227 °C | 400 - 440 °F | Injection |
Shuman 720H Black ABS Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc. |
|||
Processing Temperature | 204 - 227 °C | 400 - 440 °F | Injection |
Shuman 730 Utility White ABS Good impact strength, easy processability, good chemical resistance, good wear and abrasion resistance.Data provided by the Shuman Plastics, Inc. |
|||
Processing Temperature | 204 - 227 °C | 400 - 440 °F | Injection |
Shuman 730H White ABS Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc. |
|||
Processing Temperature | 204 - 227 °C | 400 - 440 °F | Injection |
Shuman 780H Grey ABS Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc. |
|||
Processing Temperature | 204 - 227 °C | 400 - 440 °F | |
Shuman SP810 Black Polystyrene High Impact Good impact strength, easy processability, good surface appearance, ULInformation provided by Shuman Plastics, Inc. |
|||
Processing Temperature | 204 - 227 °C | 400 - 440 °F | |
Shuman SP880 Grey Polystyrene High Impact Good impact strength, easy processability, good surface appearance, ULInformation provided by Shuman Plastics, Inc. |
|||
Processing Temperature | 204 °C | 400 °F | Optimum cure is 1 hr. @ 400°F |
Armstrong A-701 Epoxy Adhesive A one-component, light gray, thixotropic, non-sag epoxy adhesive. A-701 uses an inert oxide filler that provides excellent electrical insulation properties. Features high temperature, 400°F, bond.. |
|||
Processing Temperature | 204 °C | 400 °F | Optimum cure is 1 hr. @ 400°F |
Armstrong A-702 Epoxy Adhesive Information provided by Ellsworth Adhesives. |
|||
Processing Temperature | 204 °C | 400 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6030 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6030 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6030 NC/BK have
an excellent soft t.. |
|||
Processing Temperature | 204 °C | 400 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6040 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6040 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6040 NC/BK have
an excellent soft t.. |
|||
Processing Temperature | 204 °C | 400 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6050 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6050 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6050 NC/BK have
an excellent soft t.. |
|||
Processing Temperature | 204 °C | 400 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6060 NC Thermoplastic Elastomer (TPE) DuraGrip® DGR 6060NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6060NC has an
excellent soft touch feel,.. |
|||
Processing Temperature | 204 °C | 400 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6070 NC Thermoplastic Elastomer (TPE) DuraGrip® DGR 6070NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6070NC has an
excellent soft touch feel,.. |
|||
Processing Temperature | 204 °C | 400 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6080 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6080NC/BK are designed to be a general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR
6080NC/BK have excellent soft touc.. |
|||
Processing Temperature | 204 - 299 °C | 400 - 570 °F | Average value: 269 °C Grade Count:8 |
Overview of materials for Polycarbonate, 40% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E.. |