Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 181-55 Thermoplastic Rubber
(discontinued **) A black thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be proc.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 221-73 W175 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic UV grade elastomer designed for thin wall extrusion applications with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and c.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 251-80 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 253-50 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 281-87 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 453-45 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant wire and cable elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethy.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
ExxonMobil Santoprene® 8211-35W237 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic general purpose non-hygroscopic elastomer, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processe.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
ExxonMobil Santoprene® 151-60 Thermoplastic Rubber
(discontinued **) Description: A black thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. .. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
ExxonMobil Santoprene® 8203-45 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic general purpose non-hygroscopic elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfo.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 8281-45W237 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 8281-35W237 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 8281-55 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 8281-75 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 8281-90 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
ExxonMobil Vyram™ 9271-55 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use, as well as rubber articles in contact with non-fatty, non-oily foods as closure.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
ExxonMobil Vyram™ 9271-65 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use, as well as rubber articles in contact with non-fatty, non-oily foods as closure.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | Optimum Tunnel temperature range. |
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 75 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc.. |
|||
Processing Temperature | 177 - 260 °C | 351 - 500 °F | Profile temperatures |
NOVA Chemicals DYLARK® 238 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Processing Temperature | 177 - 216 °C | 351 - 421 °F | Extrusion |
Shuman 710 Utility Black ABS Good impact strength, easy processability, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer. |
|||
Processing Temperature | 177 - 216 °C | 351 - 421 °F | Extrusion |
Shuman 780 Grey ABS Good impact strength, easy processability, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer. |
|||
Processing Temperature | 177 - 216 °C | 351 - 421 °F | Extrusion |
Shuman 791 Black and Custom Colors ABS-Flame Retardant Long term thermal aging rated. Excellent flame retardancy, good impact strength, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer. |
|||
Processing Temperature | 177 °C | 351 °F | |
Advanced Polymer Alloys Alcryn® 2165 TR Melt Processable Rubber The 2100 Series grades of Alcryn® offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn®. The new 2100 grades bond to .. |
|||
Processing Temperature | 177 °C | 351 °F | |
Advanced Polymer Alloys Alcryn® 2170 BK Melt Processable Rubber Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 181-73 Thermoplastic Rubber
(discontinued **) A black thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be proc.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 251-92 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 281-45 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 281-55 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 281-64 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 283-40 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
Processing Temperature | 177 °C | 351 °F | Film extrusion temperature |
Dow LDPE 535I Low Density Polyethylene, Liner Grade DOW LDPE 535I resin is a barefoot general purpose liner resin with medium clarity for medium modulus packaging applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for.. |