Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 160 - 190 °C | 320 - 374 °F | Sheet Forming |
Polycasa CAST PMMA QUINN CAST has an optical transparency of 93% light transmission for transparent sheets. It is significantly lighter and much more impact resistant than glass of equivalent thickness. QUINN CAST is .. |
|||
Processing Temperature | 160 - 230 °C | 320 - 446 °F | Membranes |
Lucobit Lucobatch® 1850 T10 Polyolefin TPO Granules Lucobatch® 1850 T10 is a highly stabilized polyolefin based TPO granules. Lucobatch® 1850 T10 is employed as a master batch. Blended with suitable polyolefins, tunnel membranes are built of Lu.. |
|||
Processing Temperature | 160 - 270 °C | 320 - 518 °F | Coatings |
Lucobit Lucobatch® 1850 T100 Polyolefin TPO Granules Lucobatch® 1850 T100 is a highly stabilized polyolefin based TPO granules. Lucobatch® 1850 T100 is employed as a master batch. Blended with suitable polyolefins, tunnel membranes are built of .. |
|||
Processing Temperature | 160 - 230 °C | 320 - 446 °F | Membranes |
Lucobit Lucofin® 1411-t2 Polyolefin TPO Granules, White Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t2 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and .. |
|||
Processing Temperature | 160 - 230 °C | 320 - 446 °F | Membranes |
Lucobit Lucofin® 1414 Polyolefin TPO Granules, Silk Grey Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Processing Temperature | 160 - 270 °C | 320 - 518 °F | Extrusion |
Lucobit Lucofin® 1494 Chemically Modified Polyethylene Lucofin® 1492 is a chemically modified polyethylene, i.e. EBA grafted with maleic anhydride (MA). Lucofin® 1492 can be used pure or as a component in mixtures applications where improved polar.. |
|||
Processing Temperature | 160 °C | 320 °F | Press Cure, 10 minutes |
Mitsui MILEXâ„¢ XL-325M Phenol Aralkyl Resin, High Molecular Weight The MILEXâ„¢ Family of products is widely featured in brake systems of automobiles made by automakers through Mitsui Chemicals'. The phenolic material is primarily used as binders in brake pad.. |
|||
Processing Temperature | 160 °C | 320 °F | Hot Forming Temperature |
Spartech Polycast Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Processing Temperature | 160 °C | 320 °F | Hot Forming Temperature |
Spartech Polycast UF3 Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Processing Temperature | 160 °C | 320 °F | Hot Forming Temperature |
Spartech Polycast UF96 Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Processing Temperature | 160 - 302 °C | 320 - 576 °F | Extrusion |
Dyna-Purge® B Purging Compound Designed for Injection and Extrusion Blow MoldingGeneral Description:DYNA-PURGE B is a non-abrasive, non-chemical “engineered†thermoplastic purging compound, formulated to flow naturally .. |
|||
Processing Temperature | 160 - 302 °C | 320 - 576 °F | Extrusion |
Dyna-Purge® SF Purging Compound Designed for Sheet & Profile Co-Extrusion & Multi-Layer FilmGeneral Description:DYNA-PURGE SF is a non-abrasive, non-chemical “engineered†thermoplastic purging compound, with a proprietar.. |
|||
Processing Temperature | 160 - 180 °C | 320 - 356 °F | Mold temperature |
Sumitomo Bakelite North America 52-01 Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG.Inf.. |
|||
Processing Temperature | 160 - 180 °C | 320 - 356 °F | Mold temperature |
Sumitomo Bakelite North America RX® 2-501N Mineral Filled Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Conforms with the requirements of ASTM D5948.. |
|||
Processing Temperature | 160 - 180 °C | 320 - 356 °F | Mold temperature |
Sumitomo Bakelite North America RX® 2-520 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SI.. |
|||
Processing Temperature | 160 °C | 320 °F | Suggested baking time at this temperature is 1.5 hr. |
Von Roll Isola IMI Varnish 709 Solventless Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: 76°C. Usag.. |
|||
Processing Temperature | 160 °C | 320 °F | Cure Measuring Temperature |
Daikin DAI-EL G-952 Fluoroelastomer Terpolymer, Peroxide Curable Grade, 69% Fluorine Content Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Good solvent resistance and low-temperature characteristics.Information provided by Daikin Industrie.. |
|||
Processing Temperature | 160 - 270 °C | 320 - 518 °F | Coatings |
Lucobit Lucolit® 1310 Polyolefin TPO Granules, Grey Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi.. |
|||
Processing Temperature | 160 °C | 320 °F | Press Cure, 10 minutes |
Mitsui MILEX™ RX-2325C Low Silicone Rubber Modified Phenolic Resin
(discontinued **) The MILEX™ Family of products is widely featured in brake systems of automobiles made by the top automakers through Mitsui Chemicals' affiliation with leading brake manufacturers. The phenolic .. |