Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 20.0 - 270 °C | 68.0 - 518 °F | Average value: 185 °C Grade Count:13 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Processing Temperature | 240 - 270 °C | 464 - 518 °F | |
Gromax PBT 4130-104D 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Processing Temperature | 240 - 270 °C | 464 - 518 °F | |
Gromax PBT 5130-104 30% Glass Fiber Filled CCP Halogen-free PBT, Black. PBT flame-retarded glass fiber 30% reinforced injection molding gradeCharacteristics:Excellent electrical property Excellent temperature resistance, high heat distortion.. |
|||
Processing Temperature | 200 - 270 °C | 392 - 518 °F | |
IRPC Polimaxx Porene KU650 Acrylonitrile Butadiene Styrene Applications:injection moldingautomotive parts such as instrument panels, console boxes, switches, automotive louvers, ectelectrical appliances |
|||
Processing Temperature | 160 - 270 °C | 320 - 518 °F | Coatings |
Lucobit Lucofin® 1400MN Ethylene Butyl Acrylate Lucofin 1400MN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400MN is softer and more flexible than ethylene homopoly.. |
|||
Processing Temperature | 160 - 270 °C | 320 - 518 °F | Coatings |
Lucobit Lucofin® 1413-t3 Polyolefin TPO Granules, Dark Grey Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t3 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and .. |
|||
Processing Temperature | 230 - 270 °C | 446 - 518 °F | |
Ter Hell Plastic Terez® PBT 6750 T Polybutylene Terephthalate, Impact Modified Description: Impact modified PBT.Application: For impact stressed, injection molding parts.Information provided by Ter Hell Plastic GMBH. |
|||
Processing Temperature | 250 - 270 °C | 482 - 518 °F | |
Eurotec® Tecodur® PB70 GR15 BK EF PBT, 15% glass fiber reinforced, black, suitable for electrostatic powder coating, gas injection grade Information provided by Eurotec® |
|||
Processing Temperature | 250 - 270 °C | 482 - 518 °F | |
Eurotec® Tecomid® NB40 GR50 NL IL PA6, 50% glass fiber reinforced, impact modified, natural Information provided by Eurotec® |
|||
Processing Temperature | 250 - 270 °C | 482 - 518 °F | |
Eurotec® Tecomid® NB40 GR15 NL HS PA6, 15% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Processing Temperature | 230 - 270 °C | 446 - 518 °F | Extrusion Range |
Arkema Group Rilsamid® PA 12 AESNO MED Nylon 12 Rilsamid® AESNO MED is a rigid polyamide 12 with high viscosity designed for tube extrusion. This grade dedicated to extrusion offers the highest quality and it is specifically designed to meet the.. |
|||
Processing Temperature | 220 - 270 °C | 428 - 518 °F | Resin Temperature |
Asahi Kasei Xyron® 100V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Processing Temperature | 220 - 270 °C | 428 - 518 °F | Resin Temperature |
Asahi Kasei Xyron® 140V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Processing Temperature | 240 - 270 °C | 464 - 518 °F | Resin Temperature |
Asahi Kasei Xyron® 500V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Processing Temperature | 240 - 270 °C | 464 - 518 °F | Resin Temperature |
Asahi Kasei Xyron® 500Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Processing Temperature | 240 - 270 °C | 464 - 518 °F | Resin Temperature |
Asahi Kasei Xyron® 340V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Processing Temperature | 250 - 270 °C | 482 - 518 °F | |
Eurotec® Tecomid® NB400 GR15 NL MB PA6, 15% glass fiber reinforced, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Processing Temperature | 70.0 - 270 °C | 158 - 518 °F | Average value: 135 °C Grade Count:9 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Processing Temperature | 232 - 270 °C | 450 - 518 °F | Average value: 250 °C Grade Count:11 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |
|||
Processing Temperature | 240 - 270 °C | 464 - 518 °F | |
Gromax CCP PBT 5615-104C 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |