Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Processing Temperature = 166 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 132 - 166 °C
270 - 330 °F
Mold Temperature
Quantum Composites LYTEX® 4129 63% Glass Fiber Reinforced Epoxy SMC
LYTEX 4129 is an epoxy high performance, glass fiber reinforced ESC molding compound designed for military and aerospace structural applications requiring excellent mechanical properties, retention ..
Processing Temperature 129 - 166 °C
265 - 330 °F
Mold Temperature
Quantum Composites LYTEX® 4182 50-55% Carbon Fiber Reinforced Epoxy SMC
LYTEX 4182 is an epoxy ESC molding compound designed for structural applications requiring excellent mechanical properties, retention of properties at elevated temperatures, good chemical resistance..
Processing Temperature 129 - 166 °C
265 - 330 °F
Mold Temperature
Quantum Composites LYTEX® 4197 55% Carbon Fiber Reinforced Epoxy SMC
LYTEX 4197 is an epoxy high performance, 3K tow carbon fiber (PAN) reinforced engineered structural composite (ESC) molding compound designed for military and aerospace structural applications requi..
Processing Temperature 127 - 166 °C
260 - 330 °F
Thermoforming Temp
Alcoa KAMA 3000 High Impact Polystyrene (HIPS)  (discontinued **)
CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableMono-layer an..
Processing Temperature 127 - 166 °C
260 - 330 °F
Thermoforming Temp
Alcoa KAMA 3210 Hi-Gloss Coextruded High Impact Polystyrene  (discontinued **)
CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coat..
Processing Temperature 127 - 166 °C
260 - 330 °F
Thermoforming Temp
Alcoa KAMA 3300 Very High Impact Polystyrene  (discontinued **)
CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coat..
Processing Temperature 138 - 166 °C
280 - 330 °F
Bulk Molding Compounds BMC A30 General Purpose Molding Compound
BMC A30 is a general purpose molding compound with good dimensional stability. Due to the excellent flow and controlled reactivity, BMC A30 is well suited for injection, transfer or compression mol..
Processing Temperature 138 - 166 °C
280 - 330 °F
Bulk Molding Compounds BMC A30-3021 General Purpose Molding Compound
BMC A30-3021 is a low shrink, general purpose molding compound formulated for the lighting industry. A30-3021 is temperature stabilized for use in elevated temp. lighting applications. Due to the ..
Processing Temperature 138 - 166 °C
280 - 330 °F
Bulk Molding Compounds BMC T12-17394 General Purpose Molding Compound
BMC T12-17394 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. ..
Processing Temperature 138 - 166 °C
280 - 330 °F
Bulk Molding Compounds BMC T14 General Purpose Molding Compound
BMC T14 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T14 is well suited for injection, transfer or compression molding of intricate parts. Typica..
Processing Temperature 138 - 166 °C
280 - 330 °F
Bulk Molding Compounds BMC T15(F) High Strength Grade Molding Compound
BMC T15F is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15F is well suited for injection, transfer or compression molding..
Processing Temperature 138 - 166 °C
280 - 330 °F
Bulk Molding Compounds BMC T40(25)-XHS-15869 Die Casting Replacement Grade Molding Compound
BMC T40(25)-XHS-15869 is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical pro..
Processing Temperature 138 - 166 °C
280 - 330 °F
Bulk Molding Compounds BMC T60 Grey Wear Resistant Molding Compound
BMC T60 Grey is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cu..
Processing Temperature 138 - 166 °C
280 - 330 °F
Bulk Molding Compounds BMC T60-6002A-WG Wear Resistant Molding Compound
BMC T60-6002A-WG is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost pe..
Processing Temperature 138 - 166 °C
280 - 330 °F
Bulk Molding Compounds BMC T60-6002-WG(15) Wear Resistant Molding Compound
BMC T60-6002-WG-(15) is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cos..
Processing Temperature 138 - 166 °C
280 - 330 °F
Bulk Molding Compounds BMC T9 General Purpose Molding Compound
BMC T9 is a low cost, general purpose bulk molding compound designed for the electrical industry. It is UL listed and is used extensively in the manufacture of residential circuit breakers. BMC T9..
Processing Temperature 138 - 166 °C
280 - 330 °F
Bulk Molding Compounds BMC A20-(a) High Strength Grade Molding Compound
BMC A20 is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A20 is well suited for injection, transfer or compression molding o..
Processing Temperature 138 - 166 °C
280 - 330 °F
Bulk Molding Compounds BMC T10(GP) General Purpose Molding Compound
BMC T10(GP) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T10(GP) is well suited for injection, transfer or compression molding of intricate parts...
Processing Temperature 138 - 166 °C
280 - 330 °F
Bulk Molding Compounds BMC T12(18) General Purpose Molding Compound
BMC T12(18) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Ty..
Processing Temperature 138 - 166 °C
280 - 330 °F
Bulk Molding Compounds BMC T12-15526 General Purpose Molding Compound
BMC T12-15526 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. ..
Processing Temperature 138 - 166 °C
280 - 330 °F
Bulk Molding Compounds BMC T12-15541 General Purpose Molding Compound
BMC T12 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Typica..
Processing Temperature 127 - 166 °C
260 - 330 °F
Thermoforming Temp
Alcoa KAMA 3200 Prime High Impact Polystyrene  (discontinued **)
CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone trea..
Processing Temperature 127 - 166 °C
260 - 330 °F
Thermoforming Temp
Alcoa KAMA 3202 Freezer Modified High Impact Polystyrene  (discontinued **)
CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableColors availa..
Processing Temperature 138 - 166 °C
280 - 330 °F
Bulk Molding Compounds BMC T40(18)-LS Die Casting Replacement Grade Molding Compound
BMC T40(18)-LS is a low shrink compound designed as a direct replacement for aluminum die casting applications. T40(18)-LS is UL recognized. Excellent mechanical properties and dimensional stabili..
Processing Temperature 138 - 166 °C
280 - 330 °F
Bulk Molding Compounds BMC T40(18)V0 Die Casting Replacement Grade Molding Compound
BMC T40(18)V0 is a lower cost version of BMC T40(18) where a UL 5V rating is not necessary.
Processing Temperature 138 - 166 °C
280 - 330 °F
Bulk Molding Compounds BMC T15(GPT) General Purpose Molding Compound
BMC T15(GPT) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GPT) is well suited for injection, transfer or compression..
Processing Temperature 138 - 166 °C
280 - 330 °F
Bulk Molding Compounds BMC T40(18) Die Casting Replacement Grade Molding Compound
BMC T40(18) was formulated as a direct replacement for aluminum die casting applications. T40(18) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma..
Processing Temperature 138 - 166 °C
280 - 330 °F
Bulk Molding Compounds BMC T40(20) Die Casting Replacement Grade Molding Compound
BMC T40(20) was formulated as a direct replacement for aluminum die casting applications. T40(20) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma..
Processing Temperature 138 - 166 °C
280 - 330 °F
Bulk Molding Compounds BMC T40-4020-AQ High Strength Arc Quenching Molding Compound
BMC T40-4020-AQ was formulated as a high strength arc quenching material for electrical applications. Typical applications are arc hoods and electrical contactors.Information provided by Bulk Moldi..
Processing Temperature 138 - 166 °C
280 - 330 °F
Bulk Molding Compounds BMC T60-6009 Compression Grade Wear Resistant Molding Compound
BMC T60-6009 is a compression grade wear resistant molding compound. This material was specifically formulated for applications that require excellent abrasion resistance. Due to its low specific ..
Copyright © lookpolymers.com All Rights Reserved