Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 80.0 - 230 °C | 176 - 446 °F | Average value: 168 °C Grade Count:15 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Processing Temperature | 80.0 - 90.0 °C @Time 1800 sec |
176 - 194 °F @Time 0.500 hour |
|
Henkel Turco Scale Gon 7 Jet Engine Cleaner Turco Scale Gon 7 is an acid-activated, yellow liquid used in the Turco Jet Engine Process to condition and remove high temperature scale from jet engine parts. Approved by Rolls-Royce.Application: .. |
|||
Processing Temperature | 80.0 °C | 176 °F | Hopper Throat |
BASF Ultradur® S 4090 GX 14% Glass Filled PBT Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 14% of glass fibers for industrial parts with high dimensional stab.. |
|||
Processing Temperature | 80.0 °C | 176 °F | Hopper Throat |
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
Processing Temperature | 80.0 °C | 176 °F | Hopper throat |
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU Information provided by BASF |
|||
Processing Temperature | 80.0 °C | 176 °F | Hopper throat |
BASF Ultrason® E 3010 MR UN PESU Description: Unreinforced, higher viscosity injection molding and extrusion grade with improved toughness and chemical resistance (stress crack resistance); demolding optimized. Abbreviated designat.. |
|||
Processing Temperature | 80.0 - 366 °C | 176 - 690 °F | Average value: 320 °C Grade Count:8 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Processing Temperature | 80.0 °C | 176 °F | Hopper Throat |
BASF Ultradur® B 4300 G10 50% Glass Filled PBT Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou.. |