Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 250 °C | 482 °F | |
NYCOA 2237 Copolymer Nylon 6/66 Alloy transparent molding and extrusion gradeInformation provided by NYCOA, Inc. |
|||
Processing Temperature | 250 °C | 482 °F | |
NYCOA 870 PA 6 plasticized and heat stabilized extrusion grade for the wire jacketing industry to 3,000 fpm. UL Flammability Component listing for use as cable jacketing.Information provided by NYCOA, Inc. |
|||
Processing Temperature | 250 °C | 482 °F | mass temp |
Lehmann & Voss LUVOCOM® 1850-7315 PBT, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Processing Temperature | 250 °C | 482 °F | mass temp |
Lehmann & Voss LUVOCOM® 1850-7783-1 PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Processing Temperature | 250 °C | 482 °F | mass temp |
Lehmann & Voss LUVOCOM® 1850-7795 PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Processing Temperature | 250 °C | 482 °F | mass temp |
Lehmann & Voss LUVOCOM® 6-8395 Polyamide 12, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Especially suitable at dynamic stress situations.Electrically conductive, s.. |
|||
Processing Temperature | 250 °C | 482 °F | mass temp |
Lehmann & Voss LUVOCOM® 6-8438-1 Polyamide 12, with glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Suitable for discharging of statically generated electricity.Dynamic stressed parts.Low waterab.. |
|||
Processing Temperature | <= 250 °C | <= 482 °F | |
Kingfa FRHIPS-301 Flame Retardant Polystyrene Features:UL 94 V-1 @ 2.0 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica.. |
|||
Processing Temperature | <= 250 °C | <= 482 °F | |
Kingfa MAC-301 PC/ABS Alloy Features:Excellent balance propertiesGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingHousehold applianceAutomobile interior/exterior trim partsTel.. |
|||
Processing Temperature | 250 °C | 482 °F | mass temp |
Lehmann & Voss LUVOCOM® 1850-7581 PBT, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Processing Temperature | 250 °C | 482 °F | |
Shinil Chemical SHINNANO PA-6 Polymer Nanocomposite Engine Cover and Bumper SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using.. |
|||
Processing Temperature | 250 - 260 °C | 482 - 500 °F | AD |
UBE 1024FDX41 Nylon 6 BOPA Film Specialties: Excellent processing stabilityProcessing: Best for BOPAApplications: BOPA film (T-die)Information provided by UBE. |
|||
Processing Temperature | 250 - 290 °C | 482 - 554 °F | |
Zhejiang Juner PC-A7-5 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | <= 250 °C | <= 482 °F | |
Total HDPE HD 6081 High Density Polyethylene - Injection Molding HD 6081 is a high density polyethylene with very good organoleptic properties, rigidity and processability.It is especially suited for the production of caps & closures for non-carbonated drinks by .. |
|||
Processing Temperature | 250 - 290 °C | 482 - 554 °F | |
Zhejiang Juner PC-A2 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 250 - 270 °C | 482 - 518 °F | |
Eurotec® Tecodur® PB70 CR30 BK111 PBT, 30% carbon fiber reinforced, black Information provided by Eurotec® |
|||
Processing Temperature | 250 - 270 °C | 482 - 518 °F | |
Eurotec® Tecodur® PB70 GR15 BK EF PBT, 15% glass fiber reinforced, black, suitable for electrostatic powder coating, gas injection grade Information provided by Eurotec® |
|||
Processing Temperature | 250 - 270 °C | 482 - 518 °F | |
Eurotec® Tecomid® NB40 GR30 NL IM PA6, 30% glass fiber reinforced, impact modified, natural Information provided by Eurotec® |
|||
Processing Temperature | 250 - 270 °C | 482 - 518 °F | |
Eurotec® Tecomid® NB40 GR50 NL IL PA6, 50% glass fiber reinforced, impact modified, natural Information provided by Eurotec® |
|||
Processing Temperature | 250 - 270 °C | 482 - 518 °F | |
Eurotec® Tecomid® Nb40 GR30 NL PA6, 30% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Processing Temperature | 250 - 270 °C | 482 - 518 °F | |
Eurotec® Tecomid® NB40 KG30 NL 0G PA6, 30% glass fiber/glass bead reinforced, natural Information provided by Eurotec® |
|||
Processing Temperature | 250 - 280 °C | 482 - 536 °F | |
Gromax CCP PBT 6730-104F Glass/Mineral Filled Product Description: PBT glass/mineral reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellent w.. |