Thermal Properties Metric English Comments
Specific Heat Capacity 1.80 J/g-°C

@Temperature -17.8 °C
0.430 BTU/lb-°F

@Temperature 0.000 °F
Paratherm Corporation Paratherm™ CR Heat Transfer Fluid
Paratherm CR® heat transfer fluid is a blend of synthetic components formulated to provide superior cooling performance in closed-loop heat-transfer systems operating down to -88°C (-127°F) yet i..
Specific Heat Capacity 1.80 J/g-°C

@Temperature -17.8 °C
0.430 BTU/lb-°F

@Temperature 0.000 °F
Paratherm Corporation Paratherm™ GLT™ Heat Transfer Fluid
Paratherm GLT™ Heat Transfer Fluid is an alkylated aromatic based heat transfer fluid formulated for closed loop liquid phase heating systems to 550°F using fired heaters and to 575°F in waste-he..
Specific Heat Capacity 1.80 J/g-°C

@Temperature 100 °C
0.430 BTU/lb-°F

@Temperature 212 °F
solid; DSC
Eastman Eastman AP005 Copolyester
Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly..
Specific Heat Capacity 1.80 J/g-°C

@Temperature 100 °C
0.430 BTU/lb-°F

@Temperature 212 °F
solid; DSC
Eastman Eastman AP006 Copolyester
Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly..
Specific Heat Capacity 1.80 J/g-°C

@Temperature 100 °C
0.430 BTU/lb-°F

@Temperature 212 °F
solid; DSC
Eastman Eastman AP007 Copolyester
Applications:Automotive componentsBreathable filmsElectronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsOffice furniturePackagingPolymer modificationProfilesRubber an..
Specific Heat Capacity 1.80 J/g-°C

@Temperature -17.8 °C
0.430 BTU/lb-°F

@Temperature 0.000 °F
ConocoPhillips Hydroclear® Heat Transfer Oil
Description: Conoco Hydroclear Heat Transfer Oil is a high-quality, thermally stable inhibited oil formulated from premium Conoco hydrocracked base stocks for use in heat-transfer service. Hydroclea..
Copyright © lookpolymers.com All Rights Reserved