| Category | Fluid |
| Manufacturer | Paratherm Corporation |
| Trade Name | Paratherm™ |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Paratherm Corporation Paratherm™ GLT™ Heat Transfer Fluid.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.673 g/cc @Temperature 316 °C |
0.0243 lb/in³ @Temperature 600 °F |
|
| 0.705 g/cc @Temperature 260 °C |
0.0255 lb/in³ @Temperature 500 °F |
||
| 0.753 g/cc @Temperature 204 °C |
0.0272 lb/in³ @Temperature 400 °F |
||
| 0.785 g/cc @Temperature 149 °C |
0.0284 lb/in³ @Temperature 300 °F |
||
| 0.833 g/cc @Temperature 93.3 °C |
0.0301 lb/in³ @Temperature 200 °F |
||
| 0.865 g/cc @Temperature 37.8 °C |
0.0312 lb/in³ @Temperature 100 °F |
||
| 0.897 g/cc @Temperature -17.8 °C |
0.0324 lb/in³ @Temperature 0.000 °F |
||
| Viscosity | 0.48 cP @Temperature 249 °C |
0.48 cP @Temperature 480 °F |
|
| 0.53 cP @Temperature 238 °C |
0.53 cP @Temperature 460 °F |
||
| 0.58 cP @Temperature 227 °C |
0.58 cP @Temperature 440 °F |
||
| 0.63 cP @Temperature 216 °C |
0.63 cP @Temperature 420 °F |
||
| 0.71 cP @Temperature 204 °C |
0.71 cP @Temperature 400 °F |
||
| 0.80 cP @Temperature 193 °C |
0.80 cP @Temperature 380 °F |
||
| 0.89 cP @Temperature 182 °C |
0.89 cP @Temperature 360 °F |
||
| 1.0 cP @Temperature 171 °C |
1.0 cP @Temperature 340 °F |
||
| 1.1 cP @Temperature 160 °C |
1.1 cP @Temperature 320 °F |
||
| 1.3 cP @Temperature 149 °C |
1.3 cP @Temperature 300 °F |
||
| 1.5 cP @Temperature 138 °C |
1.5 cP @Temperature 280 °F |
||
| 1.8 cP @Temperature 127 °C |
1.8 cP @Temperature 260 °F |
||
| 2.2 cP @Temperature 116 °C |
2.2 cP @Temperature 240 °F |
||
| 2.6 cP @Temperature 104 °C |
2.6 cP @Temperature 220 °F |
||
| 3.2 cP @Temperature 93.3 °C |
3.2 cP @Temperature 200 °F |
||
| 4.2 cP @Temperature 82.2 °C |
4.2 cP @Temperature 180 °F |
||
| 5.7 cP @Temperature 71.1 °C |
5.7 cP @Temperature 160 °F |
||
| 7.8 cP @Temperature 60.0 °C |
7.8 cP @Temperature 140 °F |
||
| 12 cP @Temperature 48.9 °C |
12 cP @Temperature 120 °F |
||
| 18 cP @Temperature 37.8 °C |
18 cP @Temperature 100 °F |
||
| 30 cP @Temperature 26.7 °C |
30 cP @Temperature 80.0 °F |
||
| 54 cP @Temperature 15.6 °C |
54 cP @Temperature 60.0 °F |
||
| 106 cP @Temperature 4.44 °C |
106 cP @Temperature 40.0 °F |
||
| 254 cP @Temperature -6.67 °C |
254 cP @Temperature 20.0 °F |
||
| 720 cP @Temperature -17.8 °C |
720 cP @Temperature 0.000 °F |
||
| Molecular Weight | 330 g/mol | 330 g/mol | Average |
| Vapor Pressure | 0.00896 bar @Temperature 171 °C |
6.72 torr @Temperature 340 °F |
|
| 0.0200 bar @Temperature 193 °C |
15.0 torr @Temperature 380 °F |
||
| 0.0393 bar @Temperature 216 °C |
29.5 torr @Temperature 420 °F |
||
| 0.0758 bar @Temperature 238 °C |
56.9 torr @Temperature 460 °F |
||
| 0.131 bar @Temperature 260 °C |
98.3 torr @Temperature 500 °F |
||
| 0.221 bar @Temperature 282 °C |
166 torr @Temperature 540 °F |
||
| 0.365 bar @Temperature 304 °C |
274 torr @Temperature 580 °F |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 324 µm/m-°C | 180 µin/in-°F | converted from volume expansion |
| Specific Heat Capacity | 1.80 J/g-°C @Temperature -17.8 °C |
0.430 BTU/lb-°F @Temperature 0.000 °F |
|
| 2.01 J/g-°C @Temperature 37.8 °C |
0.480 BTU/lb-°F @Temperature 100 °F |
||
| 2.18 J/g-°C @Temperature 93.3 °C |
0.520 BTU/lb-°F @Temperature 200 °F |
||
| 2.34 J/g-°C @Temperature 149 °C |
0.560 BTU/lb-°F @Temperature 300 °F |
||
| 2.55 J/g-°C @Temperature 204 °C |
0.610 BTU/lb-°F @Temperature 400 °F |
||
| 2.72 J/g-°C @Temperature 260 °C |
0.650 BTU/lb-°F @Temperature 500 °F |
||
| 2.89 J/g-°C @Temperature 316 °C |
0.690 BTU/lb-°F @Temperature 600 °F |
||
| Thermal Conductivity | 0.0882 W/m-K @Temperature 316 °C |
0.612 BTU-in/hr-ft²-°F @Temperature 600 °F |
|
| 0.0968 W/m-K @Temperature 260 °C |
0.672 BTU-in/hr-ft²-°F @Temperature 500 °F |
||
| 0.104 W/m-K @Temperature 204 °C |
0.720 BTU-in/hr-ft²-°F @Temperature 400 °F |
||
| 0.112 W/m-K @Temperature 149 °C |
0.780 BTU-in/hr-ft²-°F @Temperature 300 °F |
||
| 0.119 W/m-K @Temperature 93.3 °C |
0.828 BTU-in/hr-ft²-°F @Temperature 200 °F |
||
| 0.128 W/m-K @Temperature 37.8 °C |
0.888 BTU-in/hr-ft²-°F @Temperature 100 °F |
||
| 0.135 W/m-K @Temperature -17.8 °C |
0.936 BTU-in/hr-ft²-°F @Temperature 0.000 °F |
||
| Maximum Service Temperature, Air | 288 °C | 550 °F | Fired Heaters |
| 302 °C | 575 °F | All Others | |
| 316 °C | 600 °F | Film Temperature | |
| Minimum Service Temperature, Air | -7.78 °C | 18.0 °F | start-up temp at 300 cPs |
| 35.0 °C | 95.0 °F | operating temp at 20 cPs | |
| Pour Point | <= -34.4 °C | <= -30.0 °F | D97 |
| Flash Point | >= 171 °C | >= 340 °F | Closed Cup (D93) |
| >= 182 °C | >= 360 °F | Open Cup (D92) |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Clear Amber Colored | |
| Base | Alkylated Aromatic | |
| Odor | Sweet |