Thermal Properties Metric English Comments
Specific Heat Capacity 1.65 J/g-°C

@Temperature 200 °C
0.394 BTU/lb-°F

@Temperature 392 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 resin. ..
Specific Heat Capacity 1.65 J/g-°C

@Temperature 50.0 °C
0.394 BTU/lb-°F

@Temperature 122 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stability..
Specific Heat Capacity 1.65 J/g-°C

@Temperature 200 °C
0.394 BTU/lb-°F

@Temperature 392 °F
ASTM C351
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 res..
Specific Heat Capacity 1.65 J/g-°C

@Temperature 50.0 °C
0.394 BTU/lb-°F

@Temperature 122 °F
ASTM C351
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)
AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stabi..
Copyright © lookpolymers.com All Rights Reserved