Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 0.113 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.473 J/g-°C

@Temperature 20.0 °C
0.113 BTU/lb-°F

@Temperature 68.0 °F
International Mold Steel PX5 Pre-Hardened Mold Steel (P20 Type)
PX5 is a modified P20, high performance, high precision, mold steel. Unique Characteristics: Exceptionally clean steel with uniform microstructure – no pin holes, inclusions or hard spots. 30-3..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 1000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 16000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 4000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 8000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 16000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 4000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 8000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 16000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 4000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 8000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, gas tungsten arc welded
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick, aged 1000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick, aged at 649°C (1200°F) for 8000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, gas tungsten arc welded, aged at 538°C (1000°F) for 4000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 427°C (800°F), aged 1000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 427°C (800°F), aged 8000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 16000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 8000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, weld metal, aged 16000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, weld metal, aged 4000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, weld metal, aged at 649°C (1200°F) for 1000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 100 °C
0.113 BTU/lb-°F

@Temperature 212 °F
International Mold Steel DHA-World Die Cast & Forging Steel
DHA-World is a high hardenability and high tough general use hot work die steel.Information provided by International Mold Steel
Specific Heat Capacity 0.472 J/g-°C

@Temperature 23.0 °C
0.113 BTU/lb-°F

@Temperature 73.4 °F
Special Metals INCOLOY® alloy 832 Stainless Steel
INCOLOY® alloy 832 is a low cost stainless steel developed specifically for domestic and industrial sheathed heater applications. With specific chemistry additions to ensure satisfactory formula..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 1000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications ..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 1000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications ..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 1000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications ..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 4000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications ..
Specific Heat Capacity 0.473 J/g-°C

@Temperature 350 °C
0.113 BTU/lb-°F

@Temperature 662 °F
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick, aged 4000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications ..
Copyright © lookpolymers.com All Rights Reserved