Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.65 J/g-°C @Temperature 200 °C |
0.394 BTU/lb-°F @Temperature 392 °F |
DSC |
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 resin. .. |
|||
Specific Heat Capacity | 1.65 J/g-°C @Temperature 50.0 °C |
0.394 BTU/lb-°F @Temperature 122 °F |
DSC |
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stability.. |
|||
Specific Heat Capacity | 1.65 J/g-°C @Temperature 200 °C |
0.394 BTU/lb-°F @Temperature 392 °F |
ASTM C351 |
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 res.. |
|||
Specific Heat Capacity | 1.65 J/g-°C @Temperature 50.0 °C |
0.394 BTU/lb-°F @Temperature 122 °F |
ASTM C351 |
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK) AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stabi.. |