Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CM6240 PC+ABS (Asia Pacific) CYCOLOY CM6240 resin is a flame retardant PC/ABS blend featuring balanced properties of high modulus, good flow and ductility. It is of Br- & Cl-free flame retardant systems intended to meet thin wa.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS (Asia Pacific) LNP* Faradex* NS003 is a compound based on PC+ABS Blend resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS (Europe-Africa-Middle East) LNP* Faradex* NS003 is a compound based on PC+ABS Blend resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubrica.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubrica.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA 6/10 (Asia Pacific) LNP* Lubricomp* QAP22S is a compound based on Nylon 6/10 resin containing PTFE, Aramid Fiber, Silicone. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA6.10 LNP* LUBRICOMP* QAP22S is a compound based on Nylon 6/10 resin containing 10% PTFE/Silicone, 10% Aramid Fiber. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature 0.000 - 90.0 °C |
35.0 µin/in-°F @Temperature 32.0 - 194 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a b.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Asia Pacific) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Asia Pacific) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Europe-Africa-Middle East) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER F-1 weathering certified in natural color, specially designed for Pool & Spa applications. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER (Asia Pacific) F-1 weathering certified in natural color, specially designed for Pool & Spa applications. Currently available in natural color only. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER (Europe-Africa-Middle East) F-1 weathering certified in natural color, specially designed for Pool & Spa applications. Currently available in natural color only. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP LNP* THERMOCOMP* MH0500C is a compound based on Polypropylene resin. Added feature of this material is: High Specific Gravity. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Chevron Phillips Xtel® XK2340 Polyphenylene Sulfide Alloy Black Polyphenylene Sulfide AlloyXtel™ XK2340 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength with an unique blend of toughness and.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Chevron Phillips Xtel® XK2240 Polyphenylene Sulfide Alloy
(discontinued **) Natural Color Polyphenylene Sulfide AlloyXtel™ XK2240 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength with an unique blend of tough.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
35.0 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G30BL BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont P.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC (Asia Pacific) LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC (Asia Pacific) LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature 23.0 - 150 °C |
35.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Americas r.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 150 °C |
35.0 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature 0.000 - 90.0 °C |
35.0 µin/in-°F @Temperature 32.0 - 194 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA)
(Unverified Data**) Amodel HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a broad.. |