Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 87.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 87.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 87.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 87.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 87.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 87.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 87.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp IF002 PA 6/12 (Asia Pacific) LNP* Thermocomp* IF002 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 87.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp IF002 PA 6/12 LNP* Thermocomp* IF002 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 87.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Europe-Africa-Middle East) Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |
|||
CTE, linear, Parallel to Flow | 87.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Europe-Africa-Middle East) Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |
|||
CTE, linear, Parallel to Flow | 87.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL FE8000S PPE+PS Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |
|||
CTE, linear, Parallel to Flow | 87.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL FE8000S PPE+PS Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |
|||
CTE, linear, Parallel to Flow | 87.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Asia Pacific) Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |
|||
CTE, linear, Parallel to Flow | 87.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Asia Pacific) Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |