Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 51.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CM8622 PC+ABS (Europe-Africa-Middle East) CYCOLOY* CM8622 is a high heat PC/ABS blend offering high modulus, low CTE and good |
|||
CTE, linear, Parallel to Flow | 51.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp DF0069E PC LNP* Thermocomp* DF0069E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied by SABIC.. |
|||
CTE, linear, Parallel to Flow | 51.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp DF0069E PC (Asia Pacific) LNP* Thermocomp* DF0069E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied by SABIC.. |
|||
CTE, linear, Parallel to Flow | 51.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP RF00AH PA 66 LNP* THERMOCOMP* RF00AH is a compound based on Nylon 66 resin containing 50% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
CTE, linear, Parallel to Flow | 51.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP RF00AH PA 66 (Asia Pacific) LNP* Thermocomp* RF00AH is a compound based on Nylon 66 resin containing Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 51.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP UF006H PPA LNP* THERMOCOMP* UF006H is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
CTE, linear, Parallel to Flow | 51.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP UF006H PPA (Asia Pacific) LNP* Thermocomp* UF006H is a compound based on Polyphthalamide resin containing Glass Fiber. |