Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Europe-Africa-Middle East) Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS (Europe-Africa-Middle East) CYCOLOY C6200 is a non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs. C6200 has improved processing window and edge crac.. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CU6800 PC+ABS (Europe-Africa-Middle East) Non-chlorinated and non-brominated flame retardant PC/ABS featuring excellent flow properties for a wide variety of applications including business equipment, TVs, monitors, enclosures, among others.. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® CX2142ME PC+ABS Cycoloy* resin grade CX2142ME is an injection moldable PC/ABS blend with Br- and Cl-free flame retardant systems. Key features of good flow, good impact, UL-94 V0 rating at 1.2 mm, and improved chem.. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS (Europe-Africa-Middle East) Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che.. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1... |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Asia Pacific) Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo.. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.2mm and 5VB at 1... |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Asia Pacific) Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer (Asia Pacific) Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS (Europe-Africa-Middle East) Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou.. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL V0150B PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a.. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Asia Pacific) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Asia Pacific) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Europe-Africa-Middle East) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA (Europe-Africa-Middle East) NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA (Asia Pacific) NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA (Europe-Africa-Middle East) NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance. |