Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 1345 °C | 2453 °F | |
Special Metals NIMONIC® Alloy 105 A precipitation-hardenable nickel-cobalt-chromium alloy with an addition of molybdenum for solid-solution strengthening. The relatively high aluminum content enhances both strength (through greater.. |
|||
Liquidus | 1345 °C | 2453 °F | |
Special Metals NIMONIC® Alloy 115 A precipitation-hardenable nickel-chromium-cobalt alloy with an addition of molybdenum for solid-solution strengthening. It is similar to NIMONIC alloy 105 but has higher levels of aluminum and tit.. |
|||
Liquidus | 1345 °C | 2453 °F | |
Special Metals NIMONIC® Alloy 901 A nickel-iron-chromium alloy containing titanium and aluminum for precipitation hardening and molybdenum for solid-solution strengthening. The alloy has high yield strength and creep resistance at .. |
|||
Liquidus | 1345 °C | 2453 °F | |
Special Metals NIMONIC® Alloy PK33 A nickel-chromium-cobalt alloy that is precipitation hardenable and also contains a relatively high (7%) level of molybdenum for solid-solution strengthening. It has an exceptional combination of h.. |