Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.10 W/m-K @Temperature 540 °C |
7.63 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Pyrotek Pyrocast AR-S Castable Refractory Pyrocast AR-S is a low cement, fused silica, castable refractory which exhibits excellent resistance to thermal shock. It is inert to liquid aluminum and its alloys. It is a high strength material.. |
|||
Thermal Conductivity | 1.10 W/m-K @Temperature 100 °C |
7.63 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast B 1 Dense Refractory Brick Description: B 1 is a fireclay quality for general applications up to 1350°CRemarks: This data represents average values, obtained from samples that were cut from standard bricks.Information prov.. |
|||
Thermal Conductivity | 1.10 W/m-K @Temperature 650 °C |
7.63 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast C Dense Refractory Brick Description: A dry-pressed fireclay brick for use up to 1250°C with a good resistance to acid slags and vapors. Application: industrial furnaces, chimneys, electrolytic reduction cells.Remarks: T.. |
|||
Thermal Conductivity | 1.10 - 1.30 W/m-K @Temperature 600 °C |
7.63 - 9.02 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURAS 60 S Moldable Refractory Material Description: Because this material contains a high percentage of sillimanite, it has a very good thermal shock resistance together with a very good slag resistance. Therefore this material finds its.. |
|||
Thermal Conductivity | 1.10 - 1.20 W/m-K @Temperature 100 °C |
7.63 - 8.33 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 160 FS Dense Refractory Castable Description: This castable is based on fused silica. It has an extremely good thermal shock resistance and minor expansion behavior up to process temperature of 900°C. Application: zinc melting f.. |
|||
Thermal Conductivity | 1.10 - 1.20 W/m-K @Temperature 100 °C |
7.63 - 8.33 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast FLUCON 140 Dense Self Flowing Refractory Castable Description: Flucon 140 is a self flowing low cement castable, based on a high quality chamotte grog.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 1.10 - 1.20 W/m-K @Temperature 100 °C |
7.63 - 8.33 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast VIBRON 140 C RAPID Dense Vibrating Refractory Castable Description: Vibron 140 C Rapid is a low cement castable, based on high quality coarse chamotte grog. Because of special additives this castable is special suited for a faster heating schedule.Remar.. |
|||
Thermal Conductivity | 1.10 - 1.20 W/m-K @Temperature 100 °C |
7.63 - 8.33 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast VIBRON 140 Dense Vibrating Refractory Castable Description: Vibron 140 is a low cement castable, based on high quality chamotte.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 1.10 W/m-K @Temperature 650 °C |
7.63 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast C Sp Dense Refractory Brick Description: A fireclay brick for use up to 1200°C.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 1.10 W/m-K @Temperature 800 °C, Time 10800 sec |
7.63 BTU-in/hr-ft²-°F @Temperature 1470 °F, Time 3.00 hour |
|
Sharadaa Ceramics REFCAST K High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Thermal Conductivity | 1.10 W/m-K @Temperature 800 °C, Time 10800 sec |
7.63 BTU-in/hr-ft²-°F @Temperature 1470 °F, Time 3.00 hour |
|
Sharadaa Ceramics REFCAST K SUPER High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Thermal Conductivity | 1.10 W/m-K @Temperature 400 °C, Time 10800 sec |
7.63 BTU-in/hr-ft²-°F @Temperature 752 °F, Time 3.00 hour |
|
Sharadaa Ceramics REFCAST LC60 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Thermal Conductivity | 1.10 W/m-K @Temperature 200 °C |
7.63 BTU-in/hr-ft²-°F @Temperature 392 °F |
Mean temp.; EN 993-15 1998 |
Skamol Group SKAMOBAR 69 Low-Alumina Fireclay Brick Low-alumina fireclay brick has the following characteristics: Max. service temperature 1100°C (2012°F)For barrier lining of aluminum reduction cellsExcellent cryolite resistanceLow thermal con.. |