Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.350 W/m-K @Temperature 23.0 °C |
2.43 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
Along flow; ISO 22007-4 |
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Thermal Conductivity | 0.350 W/m-K @Temperature 23.0 °C |
2.43 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
Along flow; ISO 22007-4 |
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp.. |
|||
Thermal Conductivity | 0.350 W/m-K @Temperature 1650 °C |
2.43 BTU-in/hr-ft²-°F @Temperature 3000 °F |
|
Zircar Zirconia FBD Zirconia Boards, Discs, and Cylinders Insulation Type FBD Boards, Discs and Cylinders are high strength, uniform, rigid, refractory structures composed of zirconia fibers stabilized with yttria. Type FBD is Zircar Zirconia's strongest and mos.. |
|||
Thermal Conductivity | 0.350 - 0.450 W/m-K @Temperature 600 °C |
2.43 - 3.12 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast GOLITE 110 Refractory Insulating Castable Description: Golite 110 is composed of a light weight refractory aggregate plus several additives to improve the mechanical and refractory properties.Remarks: These values apply to cast products. Al.. |
|||
Thermal Conductivity | 0.350 - 0.450 W/m-K @Temperature 100 °C |
2.43 - 3.12 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast GOLITE 125 Refractory Insulating Castable Description: This insulating castable is characterized by a good mechanical strength and thermal shock resistance.Remarks: These values apply to cast products. Also available in gunning variety, mar.. |
|||
Thermal Conductivity | 0.350 - 0.450 W/m-K @Temperature 100 °C |
2.43 - 3.12 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast GOLITE 140 Refractory Insulating Castable Description: This castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere.Remarks:.. |
|||
Thermal Conductivity | 0.350 W/m-K @Temperature 1650 °C |
2.43 BTU-in/hr-ft²-°F @Temperature 3000 °F |
|
Zircar Zirconia FBD Zirconia Boards, Discs, and Cylinders Insulation Type FBD Boards, Discs and Cylinders are high strength, uniform, rigid, refractory structures composed of zirconia fibers stabilized with yttria. Type FBD is Zircar Zirconia's strongest and mos.. |
|||
Thermal Conductivity | 0.350 W/m-K @Temperature 538 °C |
2.43 BTU-in/hr-ft²-°F @Temperature 1000 °F |
ASTM C182 |
BNZ Materials BNZ-28 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.350 W/m-K @Temperature 800 °C |
2.43 BTU-in/hr-ft²-°F @Temperature 1470 °F |
ASTM C182 |
BNZ Materials BNZP-26 Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.350 W/m-K @Temperature 800 °C |
2.43 BTU-in/hr-ft²-°F @Temperature 1470 °F |
ASTM C182 |
BNZ Materials BNZP-26HS Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.350 W/m-K @Temperature 800 °C |
2.43 BTU-in/hr-ft²-°F @Temperature 1470 °F |
ASTM C182 |
BNZ Materials Color B Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.350 W/m-K @Temperature 1093 °C |
2.43 BTU-in/hr-ft²-°F @Temperature 1999 °F |
ASTM C182 |
BNZ Materials PA 20 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.350 W/m-K @Temperature 816 °C |
2.43 BTU-in/hr-ft²-°F @Temperature 1500 °F |
ASTM C182 |
BNZ Materials PA 23 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.350 W/m-K @Temperature 538 °C |
2.43 BTU-in/hr-ft²-°F @Temperature 1000 °F |
ASTM C182 |
BNZ Materials PA 26 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.350 - 0.450 W/m-K @Temperature 600 °C |
2.43 - 3.12 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast GOLITE MW Refractory Insulating Castable Description: Golite MW (medium weight) is composed of a light weight refractory aggregate plus several additives to improve the mechanical properties.Remarks: These values apply to cast products. Al.. |
|||
Thermal Conductivity | 0.350 - 0.450 W/m-K @Temperature 100 °C |
2.43 - 3.12 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast GOLITE 140 GM Refractory Insulating Castable Description: This gunning castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere... |