Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.220 W/m-K @Temperature 871 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 1600 °F |
|
Pyrotek Pyrocast L-30 Moldable Refractory Pyrocast L-30 is a refractory moldable designed for use in contact with molten aluminum. Pyrocast L-30 has excellent workability for use as an insulating lining or patching material and is recommen.. |
|||
Thermal Conductivity | 0.220 W/m-K @Temperature 1100 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Zircar Zirconia ZYFB-6 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Thermal Conductivity | 0.220 W/m-K @Temperature 250 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 482 °F |
ASTM E1530 |
3M Dyneon™ CCX6380 PTFE, 10% Polyimide Filler
(discontinued **) Type II, free flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon div.. |
|||
Thermal Conductivity | 0.220 W/m-K @Temperature 100 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E831 |
3M Dyneon™ TFM™ 1705 Modified PTFE Powder
(discontinued **) Type II, gr. 1 PTFE. Dyneon™ TFM™ 1705 PTFE is a second-generation modified polytetrafluoro-ethylene (PTFE) that maintains the exceptional chemical and heat resistance properties of first-generat.. |
|||
Thermal Conductivity | 0.220 - 0.300 W/m-K @Temperature 100 °C |
1.53 - 2.08 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast GOLITE 1.2.4. Mix Refractory Insulating Castable Description: This lightweight castable is composed of 1 part cement, 2 parts light weight grains and 4 parts vermiculite. Special additives provide for higher strength and less shrinkage.Remarks: Th.. |
|||
Thermal Conductivity | 0.220 W/m-K @Temperature 982 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 1800 °F |
|
ICHS Fiberfax® Alumina-Silica Ceramic Fibers Fiberfrax® ceramic fibers are made from high-purity alumina-silica materials. ICHS uses Fiberfrax® ceramic fiber to manufacture vacuum-formed products in:High-Temperature DuctworkCombustion C.. |
|||
Thermal Conductivity | 0.220 - 0.320 W/m-K @Temperature 600 °C |
1.53 - 2.22 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast GOLITE 120 Refractory Insulating Castable Description: Golite 120 is composed of light weight aggregates, alumina cement and special additions to be sure of a high strength and a low firing shrinkage.Remarks: These values apply to cast prod.. |
|||
Thermal Conductivity | 0.220 - 0.300 W/m-K @Temperature 950 °C |
1.53 - 2.08 BTU-in/hr-ft²-°F @Temperature 1740 °F |
|
Gouda Vuurvast GOLITE 95 Refractory Insulating Castable Description: Golite 95 is widely applied as an insulating backlining behind a dense castable, especially in the petrochemical industry.Remarks: These values apply to cast products. Also available in.. |
|||
Thermal Conductivity | 0.220 W/m-K @Temperature 400 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 752 °F |
ASTMÂ C-201 supplemented by ASTM C-182 |
Skamol Group SKAMOCAST 112-80 Insulating Castable SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f.. |
|||
Thermal Conductivity | 0.220 W/m-K @Temperature 1100 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Zircar Ceramics AL-25/1700 Alumina Insulation AL-25/1700 is a rigid medium duty grade of alumina fiber board. Not as strong as SALI but capable of delivering years of service.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.221 W/m-K @Temperature 871 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 1600 °F |
|
Zircar Ceramics AX Moldable Alumina-Silica Insulation AX Moldable is a sticky fiber rich paste useful to obtain a hard surface coating, bond alumina-silica fiber based insulation products to themselves and to form complex shapes for use to 1260°C (230.. |
|||
Thermal Conductivity | 0.220 W/m-K @Temperature 1100 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Zircar Ceramics AXL Alumina-Silica Insulation ZIRCAR Alumina Silica Insulation Type AXL and Type AXHTM are inorganically bound insulation boards typified by their rigid outer surfaces and unbound interiors. They offer low thermal conductivity a.. |
|||
Thermal Conductivity | 0.220 W/m-K @Temperature 1250 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 2280 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics ZAL-15AA Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.220 W/m-K @Temperature 1100 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 2010 °F |
parallel to thickness |
Zircar Ceramics Z-MAG/2300 Soluble Fiber Insulation ZIRCAR NON-RCF Insulation Type Z-MAG/2300 is a rigid combination of soluble NON-RCF silica magnesia glass fibers and inorganic binder. It is suitable for use as a substitute for insulation containin.. |
|||
Thermal Conductivity | 0.220 W/m-K @Temperature 1010 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 1850 °F |
|
Zircar Refractory Composites RSBD-HD ALUMINA-SILICA INSULATION ZRCI Alumina-Silica Insulation Type RSBD-HD Board is a ceramic fiber insulation suitable for use to 1260°C (2300°C). It is a strong, rigid refractory structure of high temperature ceramic fibers a.. |
|||
Thermal Conductivity | 0.220 W/m-K @Temperature 1100 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Zircar Zirconia ZYFB-6 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Thermal Conductivity | 0.220 W/m-K @Temperature 816 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 1500 °F |
ASTM C182 |
BNZ Materials BNZ-20 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.220 W/m-K @Temperature 538 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 1000 °F |
ASTM C182 |
BNZ Materials BNZ-23HS Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.220 W/m-K @Temperature 600 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTM C182 |
BNZ Materials BNZP-23 Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.220 W/m-K @Temperature 800 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 1470 °F |
ASTM C182 |
BNZ Materials BNZP-23L Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.220 W/m-K @Temperature 260 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 500 °F |
ASTM C182 |
BNZ Materials C-22 Z Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.220 W/m-K @Temperature 100 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM D1530 |
3M Dyneon™ TFM™ 1700 Modified PTFE Powder Type III, gr. 1 PTFE. Dyneon™ TFM™ 1700 PTFE is a second-generation modified polytetrafluoro-ethylene (PTFE) that maintains the exceptional chemical and heat resistance properties of first-genera.. |
|||
Thermal Conductivity | 0.220 W/m-K @Temperature 1350 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 2460 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics ZAL-15 Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |