Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0700 W/m-K @Temperature 295 °C |
0.486 BTU-in/hr-ft²-°F @Temperature 563 °F |
|
Pyrotek AL-THERM 2100H Vacuum formed refractories for use with modular hot top systems Pyrotek offers a variety of vacuum formed products composed from Al-Therm 2100H. These alumina-silicate fibers feature a unique inorganic binder system and are custom designed to shapes which are f.. |
|||
Thermal Conductivity | 0.0700 W/m-K @Temperature 204 °C |
0.486 BTU-in/hr-ft²-°F @Temperature 399 °F |
|
Pyrotek I-14 Insulating Board Pyrotek's I-14 is a low density hydrous calcium silicate board which features exceptional strength and low thermal conductivity. Inorganic and incombustible, I-14 also contains no RDF's.A.. |
|||
Thermal Conductivity | 0.0700 W/m-K @Temperature 204 °C |
0.486 BTU-in/hr-ft²-°F @Temperature 399 °F |
|
Pyrotek PTB 2200 Structural Board ApplicationsCaster tips Small machined nozzles Slotted caster tips AdvantagesHigh strength Resistant to thermal shock Easily machined Non-wetting to molten non-ferrous metals Low thermal mass High t.. |
|||
Thermal Conductivity | 0.0700 W/m-K @Temperature 260 °C |
0.486 BTU-in/hr-ft²-°F @Temperature 500 °F |
|
Pyrotek Pyrotherm TF-19 Lightweight, non-RCF insulation board for ovens, furnaces, kilns and vessels Pyrotherm TF-19 is a high-temperature board providing high strength and excellent workability. It is composed of mineral fiber and selected mineral additives.ApplicationsPot cradle insulation (for .. |
|||
Thermal Conductivity | 0.0700 W/m-K @Temperature 300 °C |
0.486 BTU-in/hr-ft²-°F @Temperature 572 °F |
@ 110 kg/m³; ASTM C177, ISO 8302, DIN EN-12667:2001-05 |
Microtherm Group MT Thermosphere® Moldable Insulation Paste MT Thermosphere® is a low density temperature resistant paste with excellent thermal insulation properties from cryogenic to high temperature exposure. It is a perfectly seamless insulation syste.. |
|||
Thermal Conductivity | 0.0700 W/m-K @Temperature 200 °C |
0.486 BTU-in/hr-ft²-°F @Temperature 392 °F |
Mean temp.; ASTMÂ C-182 |
Skamol Group SUPER 1100 E Calcium Silicate Insulating Slab SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity.. |
|||
Thermal Conductivity | 0.0700 W/m-K @Temperature 200 °C |
0.486 BTU-in/hr-ft²-°F @Temperature 392 °F |
Mean temp.; ASTMÂ C-182 |
Skamol Group SUPER 1100 ET Calcium Silicate Insulating Slab SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity.. |
|||
Thermal Conductivity | 0.0700 W/m-K @Temperature 315 °C |
0.486 BTU-in/hr-ft²-°F @Temperature 599 °F |
parallel to thickness; ASTM C177-76 |
Zircar Ceramics AB Alumina Blanket Two varieties of quilted alumina fiber blanket that have good handleability and offer very low thermal conductivity. These resilient blankets are easily cut and applied to numerous application with .. |
|||
Thermal Conductivity | 0.0700 W/m-K @Temperature 400 °C |
0.486 BTU-in/hr-ft²-°F @Temperature 752 °F |
parallel to thickness; ASTM C177-76 |
Zircar Ceramics ALC Alumina Insulation ALC is the same material as ZAL-15 - but brings exceptional uniformity in an insulation material in cylindrical form.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.0700 W/m-K @Temperature 315 °C |
0.486 BTU-in/hr-ft²-°F @Temperature 599 °F |
parallel to thickness; ASTM C177-76 |
Zircar Ceramics MB Alumina Blanket Two varieties of quilted alumina fiber blanket that have good handleability and offer very low thermal conductivity. These resilient blankets are easily cut and applied to numerous application with .. |
|||
Thermal Conductivity | 0.0700 W/m-K @Temperature 400 °C |
0.486 BTU-in/hr-ft²-°F @Temperature 752 °F |
ASTM C177-76 |
Zircar Ceramics Uniform A1 Alumina-Silica Insulation ZIRCAR Alumina-Silica Insulation Type "UNIFORM A" is a family of refractory ceramic fiber based insulations with exceptional machineability and strength. They are made of specially prepared alumi.. |
|||
Thermal Conductivity | 0.0700 W/m-K @Temperature 315 °C |
0.486 BTU-in/hr-ft²-°F @Temperature 599 °F |
parallel to thickness; ASTM C177 |
Zircar Refractory Composites RSMAT-3000 ALUMINA MAT ZRCI Type RSMAT-3000 is a high purity, high temperature, flexible form composed of continuous 97% alumina ceramic fibers designed for use to 1650°C (3002°F). Type RSMAT-3000 contains little shot a.. |
|||
Thermal Conductivity | 0.0700 W/m-K @Temperature 200 °C |
0.486 BTU-in/hr-ft²-°F @Temperature 392 °F |
parallel to thickness |
Zircar Refractory Composites ZIRCAL-18 Refractory Board Type ZIRCAL-18 Refractory Board is a high temperature calcium silicate block insulation with excellent mechanical properties and stability up to 1100°C(2000°F). Its high thermal insulating value m.. |
|||
Thermal Conductivity | 0.0700 W/m-K @Temperature 315 °C |
0.486 BTU-in/hr-ft²-°F @Temperature 599 °F |
parallel to thickness; ASTM C177-76 |
Zircar Ceramics Alumina Mat A layered, low density flexible mat made of 100% polycrystalline alumina fiber (non-RCF) designed for use to temperatures as high as 1650°C (3002°F). Shot free low density mat used as fill between.. |
|||
Thermal Conductivity | 0.0700 W/m-K @Temperature 200 °C |
0.486 BTU-in/hr-ft²-°F @Temperature 392 °F |
parallel to thickness; ASTM C177 |
Zircar Refractory Composites RS-B ALUMINA-SILICA MOLDABLE ZIRCAR Alumina-Silica Insulating Blanket Type RS-B Moldable is composed of long, high strength ceramic fibers, with an inorganic alumina binder/rigidizing agent. It is a wet blanket that is shipped .. |
|||
Thermal Conductivity | 0.0700 W/m-K @Temperature 200 °C |
0.486 BTU-in/hr-ft²-°F @Temperature 392 °F |
ASTM C182 |
BNZ Materials Zelieblok 2000S Structural Ceramic Insulation Information provided by BNZ Materials Inc. |
|||
Thermal Conductivity | 0.0700 W/m-K @Temperature 400 °C |
0.486 BTU-in/hr-ft²-°F @Temperature 752 °F |
parallel to thickness; ASTM C177-76 |
Zircar Ceramics ALCAA Alumina Insulation ALC is the same material as ZAL-15 - but brings exceptional uniformity in an insulation material in cylindrical form.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.0700 W/m-K @Temperature 300 °C |
0.486 BTU-in/hr-ft²-°F @Temperature 572 °F |
ASTM C177-76 |
Zircar Ceramics ASH Alumina-Silica Insulation ZIRCAR Ceramics Alumina-Silica Insulation Type ASH is one of the first alumina-silica products produced by ZIRCAR. Made of bulk fiber and inorganic alumina binders Type ASH is uniform throughout its.. |