Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 12.6 W/m-K @Temperature 200 °C |
87.4 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Waspaloy™ alloy, sheet Age-hardenable superalloy with very good strength at temperatures up 980°C (1800°F), can be cold-formed in the annealed condition, may also be hot formed at 1040°C (1900°F) and above, go.. |
|||
Thermal Conductivity | 12.6 W/m-K @Temperature 200 °C |
87.4 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Thermal Conductivity | 12.6 W/m-K @Temperature 200 °C |
87.4 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Thermal Conductivity | 12.6 W/m-K @Temperature 200 °C |
87.4 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Thermal Conductivity | 12.6 W/m-K @Temperature 200 °C |
87.4 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Thermal Conductivity | 12.6 W/m-K @Temperature 200 °C |
87.4 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Thermal Conductivity | 12.6 W/m-K @Temperature 200 °C |
87.4 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Thermal Conductivity | 12.6 W/m-K @Temperature 150 °C, Time 3600 sec |
87.4 BTU-in/hr-ft²-°F @Temperature 302 °F, Time 1.00 hour |
|
Epoxy Technology EPO-TEK® EK1000 Epoxy Material Description: A single component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance making it ideal for the demanding .. |
|||
Thermal Conductivity | 12.6 W/m-K @Temperature 150 °C, Time 3600 sec |
87.4 BTU-in/hr-ft²-°F @Temperature 302 °F, Time 1.00 hour |
|
Epoxy Technology EPO-TEK® EK1000-MP Epoxy Material Description: A single component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance making it ideal for the demanding .. |
|||
Thermal Conductivity | 12.6 W/m-K @Temperature 150 °C, Time 3600 sec |
87.4 BTU-in/hr-ft²-°F @Temperature 302 °F, Time 1.00 hour |
|
Epoxy Technology EPO-TEK® EK2000 Epoxy Preliminary Product Information SheetMaterial Description: A two component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance .. |
|||
Thermal Conductivity | 12.6 W/m-K @Temperature 204 °C |
87.4 BTU-in/hr-ft²-°F @Temperature 399 °F |
|
ATI Allegheny Ludlum AL 625HP™ Stainless Steel Nickel-based superalloy. Characteristics:exceptional fatigue resistance, excellent resistance to oxidation and corrosion, outstanding strength and toughness over a range of temperatures from cryogen.. |