Polymer Property : Thermal Conductivity = 0.400 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.400 W/m-K

@Temperature 100 °C
2.78 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1530
3M Dyneon™ CC655 PTFE, 50% Stainless Steel Filled  (discontinued **)
Type II, free flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon div..
Thermal Conductivity 0.400 - 0.500 W/m-K

@Temperature 600 °C
2.78 - 3.47 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast FI 45-12 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.400 - 0.500 W/m-K

@Temperature 600 °C
2.78 - 3.47 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast GOLITE 125 Refractory Insulating Castable
Description: This insulating castable is characterized by a good mechanical strength and thermal shock resistance.Remarks: These values apply to cast products. Also available in gunning variety, mar..
Thermal Conductivity 0.400 - 0.500 W/m-K

@Temperature 600 °C
2.78 - 3.47 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast GOLITE 140 Refractory Insulating Castable
Description: This castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere.Remarks:..
Thermal Conductivity 0.400 - 0.500 W/m-K

@Temperature 100 °C
2.78 - 3.47 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast GOLITE 160 Refractory Insulating Castable
Description: This castable can be used up to very high temperatures under reducing conditions.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information..
Thermal Conductivity 0.400 W/m-K

@Temperature 1093 °C
2.78 BTU-in/hr-ft²-°F

@Temperature 1999 °F
ASTM C182
BNZ Materials BNZ-25 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.400 W/m-K

@Temperature 1093 °C
2.78 BTU-in/hr-ft²-°F

@Temperature 1999 °F
ASTM C182
BNZ Materials BNZ-26 HS Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.400 W/m-K

@Temperature 260 °C
2.78 BTU-in/hr-ft²-°F

@Temperature 500 °F
ASTM C182
BNZ Materials BNZ-3000 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.400 W/m-K

@Temperature 1000 °C
2.78 BTU-in/hr-ft²-°F

@Temperature 1830 °F
ASTM C182
BNZ Materials BNZP-26HS Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.400 W/m-K

@Temperature 1000 °C
2.78 BTU-in/hr-ft²-°F

@Temperature 1830 °F
ASTM C182
BNZ Materials Color B Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.400 W/m-K

@Temperature 800 °C
2.78 BTU-in/hr-ft²-°F

@Temperature 1470 °F
ASTM C182
BNZ Materials Color CA Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.400 - 0.500 W/m-K

@Temperature 1000 °C
2.78 - 3.47 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast FI 25-12 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.400 - 0.500 W/m-K

@Temperature 600 °C
2.78 - 3.47 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast GOLITE 135 GM Refractory Insulating Castable
Description: This gunning material can be used in direct contact with open fire and has a high strength.Remarks: These values were obtained from cast samples. These values apply to cast products.Inf..
Thermal Conductivity 0.400 - 0.500 W/m-K

@Temperature 600 °C
2.78 - 3.47 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast GOLITE 140 GM Refractory Insulating Castable
Description: This gunning castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere...