Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Dyneon™ CC655 PTFE, 50% Stainless Steel Filled  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ CC655 PTFE, 50% Stainless Steel Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Type II, free flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon division of 3M.
Physical Properties Metric English Comments
Specific Gravity 3.33 g/cc
3.33 g/cc
ASTM D4894
Bulk Density 1.10 g/cc
0.0397 lb/in³
ASTM D4894
Particle Size 750 µm
750 µm
ASTM D4894
Deformation 3.0 %

@Pressure 15.00 MPa
3.0 %

@Pressure 2175 psi
permanent; ASTM D621
5.0 %

@Time 86400 sec,
Pressure 15.00 MPa
5.0 %

@Time 24.0 hour,
Pressure 2175 psi
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 71
71
Initial; ASTM D2240
65

@Time 15.0 sec
65

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 20.7 MPa
3000 psi
ASTM D4894
Elongation at Break 220 %
220 %
ASTM D4894
Tensile Modulus 0.176 GPa
25.5 ksi
ASTM D638
Thermal Properties Metric English Comments
CTE, linear 82.8 µm/m-°C

@Temperature 30.0 - 100 °C
46.0 µin/in-°F

@Temperature 86.0 - 212 °F
ASTM E831
113 µm/m-°C

@Temperature 100 - 200 °C
63.0 µin/in-°F

@Temperature 212 - 392 °F
ASTM E831
140 µm/m-°C

@Temperature 200 - 300 °C
78.0 µin/in-°F

@Temperature 392 - 572 °F
ASTM E831
Thermal Conductivity 0.390 W/m-K

@Temperature 250 °C
2.71 BTU-in/hr-ft²-°F

@Temperature 482 °F
ASTM E1530
0.400 W/m-K

@Temperature 100 °C
2.78 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1530
Shrinkage 1.6 %
1.6 %
ASTM D4894
Users viewing this material also viewed the following: