Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.290 W/m-K @Temperature 538 °C |
2.01 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Pyrotek NAD-1000 High Temperature Engineering Board NAD-1000 is a high density calcium silicate board reinforced with selected fibers to produce excellent thermal characteristics and dimensional stability up to 1000°C. NAD-1000 retains high strengt.. |
|||
Thermal Conductivity | 0.290 W/m-K @Temperature 23.0 °C |
2.01 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
Average; ISO/CD 22007-4 |
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia.. |
|||
Thermal Conductivity | 0.290 W/m-K @Temperature 100 °C |
2.01 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1530 |
3M Dyneon™ CCX1029 PTFE, 10% Carbon Fiber Filled
(discontinued **) Type I, non-free-flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon .. |
|||
Thermal Conductivity | 0.290 W/m-K @Temperature 100 °C |
2.01 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1530 |
3M Dyneon™ CC605 PTFE 25% Fiberglass Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon. |
|||
Thermal Conductivity | 0.290 - 0.390 W/m-K @Temperature 600 °C |
2.01 - 2.71 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast GI 26 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.290 - 0.390 W/m-K @Temperature 1200 °C |
2.01 - 2.71 BTU-in/hr-ft²-°F @Temperature 2190 °F |
|
Gouda Vuurvast GOLITE 120 Refractory Insulating Castable Description: Golite 120 is composed of light weight aggregates, alumina cement and special additions to be sure of a high strength and a low firing shrinkage.Remarks: These values apply to cast prod.. |
|||
Thermal Conductivity | 0.290 W/m-K @Temperature 600 °C |
2.01 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTMÂ C-182 |
Skamol Group VIP 12 Vermiculite Insulating Slab SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr.. |
|||
Thermal Conductivity | 0.290 W/m-K @Temperature 1650 °C |
2.01 BTU-in/hr-ft²-°F @Temperature 3000 °F |
|
Zircar Refractory Composites RS-99-45 Refractory Sheet ZRCI Refractory Sheet Type RS-99-45 is comprised of 99% alumina. This "All-Alumina" material is strong, uniform, rigid, refractory structure composed of alpha alumina fibers and high purity inorgani.. |
|||
Thermal Conductivity | 0.290 W/m-K @Temperature 600 °C |
2.01 BTU-in/hr-ft²-°F @Temperature 1110 °F |
parallel to thickness |
Zircar Refractory Composites ZIRCAL-95 Refractory Board Type ZIRCAL-95 Refractory Board is produced from a combination of natural organic fibers and inert reinforcing fillers in a high density calcium silicate hydrate matrix. Designed as a substitute for.. |
|||
Thermal Conductivity | 0.290 W/m-K @Temperature 1093 °C |
2.01 BTU-in/hr-ft²-°F @Temperature 1999 °F |
8 pcf blanket (Parallel to Thickness) |
Zircar Ceramics ASB-2300 Alumina-Silica Blanket Useful to temperatures of 1260°C this mechanically needled ceramic fiber blanket is available in a variety of thickness' and densities. Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.290 W/m-K @Temperature 1093 °C |
2.01 BTU-in/hr-ft²-°F @Temperature 1999 °F |
8 pcf blanket (Parallel to Thickness) |
Zircar Ceramics ASB-2600 Alumina-Silica Blanket Useful to temperatures of 1400°C this mechanically needled ceramic fiber blanket is available in a variety of thickness' and densities. Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.290 W/m-K @Temperature 1093 °C |
2.01 BTU-in/hr-ft²-°F @Temperature 1999 °F |
ASTM C182 |
BNZ Materials BNZ-23HS Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.290 W/m-K @Temperature 538 °C |
2.01 BTU-in/hr-ft²-°F @Temperature 1000 °F |
ASTM C182 |
BNZ Materials BNZ-26-60 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.290 W/m-K @Temperature 1000 °C |
2.01 BTU-in/hr-ft²-°F @Temperature 1830 °F |
ASTM C182 |
BNZ Materials BNZP-26A Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.290 W/m-K @Temperature 200 °C |
2.01 BTU-in/hr-ft²-°F @Temperature 392 °F |
ASTM C182 |
BNZ Materials Color CA Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.290 W/m-K @Temperature 538 °C |
2.01 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
BNZ Materials CS85 High Temperature Structural Insulation NZ manufactures a variety of non-asbestos calcium silicate structural insulations that combine high strength and excellent thermal insulating characteristics for use in a variety of heat processing,.. |
|||
Thermal Conductivity | 0.290 W/m-K @Temperature 538 °C |
2.01 BTU-in/hr-ft²-°F @Temperature 1000 °F |
ASTM C182 |
BNZ Materials PA 23 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |