Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 84.0 °C @Load 5.001 kg |
183 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PP HBK15030 D Polypropylene, Multifiller High Gloss, Detergent Resistant Information provided by Polykemi AB |
|||
Vicat Softening Point | 84.0 °C @Load 5.001 kg |
183 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PP HBK15030 Polypropylene, Multifiller High Gloss Information provided by Polykemi AB |
|||
Vicat Softening Point | 84.0 °C @Load 5.001 kg |
183 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH TS15020 D Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 84.0 °C @Load 5.001 kg |
183 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH TS15020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 84.0 °C @Load 5.001 kg |
183 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH TS15040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 84.0 °C @Load 5.001 kg |
183 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH TS2020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 84.0 °C @Load 5.001 kg |
183 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH TS4020D Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant Information provided by Polykemi AB |
|||
Vicat Softening Point | 84.0 °C @Load 5.001 kg |
183 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPHC T5040 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 84.0 °C @Load 5.001 kg |
183 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPHC T8040 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 84.0 °C @Load 5.001 kg |
183 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH BK901010 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 84.0 °C @Load 5.00 kg |
183 °F @Load 11.0 lb |
50°C/min; ASTM D1525 |
Kingfa HF-606 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmHigh flowModerate UV stabilityHigh stiffnessApplications:Injection moldingMonitor cabinetCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co.,.. |
|||
Vicat Softening Point | 84.0 °C @Load 5.00 kg |
183 °F @Load 11.0 lb |
50°C/min; ASTM D1525 |
Kingfa HF-626 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmHigh flowHigh impact resistanceApplications:Injection moldingMonitor cabinetCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Vicat Softening Point | 84.0 °C @Load 5.00 kg |
183 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTASTIR GP 1000 Polystyrene Polystyrene crystal, general purposeGood melt flow rate, stiffness, gloss, excellent transparencyInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 84.0 °C @Load 5.00 kg |
183 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
Chi Mei Polylac® PA-764 ABS - Flame Retardant F.R. Weather Resistant |
|||
Vicat Softening Point | 84.0 °C @Load 5.001 kg |
183 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PP HBK1501515 Polypropylene, Multifiller High Gloss Information provided by Polykemi AB |
|||
Vicat Softening Point | 84.0 °C @Load 5.001 kg |
183 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH TS3020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 84.0 °C @Load 5.001 kg |
183 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH TS4020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 84.0 °C @Load 5.001 kg |
183 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH TS4040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 84.0 °C @Load 5.001 kg |
183 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH TS5040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 84.0 °C @Load 5.001 kg |
183 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH TS5040DS Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant Information provided by Polykemi AB |
|||
Vicat Softening Point | 84.0 °C @Load 5.001 kg |
183 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH TS8020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 84.0 °C @Load 5.001 kg |
183 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH TS8038 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 84.0 °C @Load 5.001 kg |
183 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPHC T11030 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 84.0 °C @Load 5.001 kg |
183 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH TS2040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |